Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.070 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.177 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.45 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa2Si + CaBr2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 -1> | 285.0 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 272.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 182.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 255.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 109.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 292.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 292.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 292.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 73.1 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 73.1 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 228.0 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 220.8 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 212.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 182.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 219.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 328.7 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 273.8 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 293.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 255.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 182.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 109.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 219.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 219.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 182.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 255.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 255.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 182.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 292.2 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 98.0 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 255.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 255.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 182.6 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 272.7 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 328.7 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 219.0 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 294.4 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 73.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 228.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 255.7 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 285.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 219.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 219.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 328.7 |
GaSe (mp-1943) | <1 0 1> | <1 0 -1> | 285.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 182.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 219.2 |
BN (mp-984) | <1 1 1> | <0 1 0> | 272.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 73.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 292.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 219.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2Pt3O8 (mp-8710) | 0.6385 | 0.000 | 3 |
YZrO3 (mp-766243) | 0.6160 | 0.091 | 3 |
Lu2TiO5 (mp-754073) | 0.6371 | 0.040 | 3 |
Ca3SiBr2 (mp-568791) | 0.3164 | 0.183 | 3 |
Sm3Bi5O12 (mp-757507) | 0.6397 | 0.028 | 3 |
CaLa2BiO6 (mvc-15176) | 0.6674 | 0.079 | 4 |
Li2FeWO6 (mp-776913) | 0.6258 | 0.080 | 4 |
Li3Fe(SbO3)4 (mp-772701) | 0.6661 | 0.066 | 4 |
Li3Mn(SbO3)4 (mp-771739) | 0.6690 | 0.064 | 4 |
Mn2FeWO6 (mp-1078277) | 0.6703 | 0.104 | 4 |
Te2Ir (mp-569322) | 0.6343 | 0.015 | 2 |
Te2Ir (mp-569388) | 0.6394 | 0.004 | 2 |
Zn3N2 (mp-9460) | 0.6577 | 0.000 | 2 |
IrSe2 (mp-1361) | 0.6700 | 0.000 | 2 |
Te2Ir (mp-1551) | 0.6353 | 0.000 | 2 |
Li4MnCr(WO6)2 (mp-761370) | 0.6965 | 0.072 | 5 |
Li4Fe2TeWO12 (mp-768021) | 0.6629 | 0.075 | 5 |
Li4Cr2TeWO12 (mp-775566) | 0.6603 | 0.080 | 5 |
Li4Mn2TeWO12 (mp-768044) | 0.6522 | 0.059 | 5 |
Li4TiMn(WO6)2 (mp-770980) | 0.6815 | 0.037 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Si Br |
Final Energy/Atom-3.5286 eV |
Corrected Energy-21.1717 eV
-21.1717 eV = -21.1717 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)