material

Si5Rh4

ID:

mp-568792

DOI:

10.17188/1274696


Tags: Rhodium silicide (4/5)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.732 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.02 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21/m [11]
Hall
-P 2yb
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 24355 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
PbSe (mp-2201) <1 0 0> <1 0 0> 0.000 310.1
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.000 310.1
GaSb (mp-1156) <1 0 0> <1 0 0> 0.006 310.1
SiC (mp-11714) <1 1 0> <1 1 1> 0.010 270.6
KP(HO2)2 (mp-23959) <1 0 1> <1 0 -1> 0.017 137.0
CdSe (mp-2691) <1 0 0> <1 0 0> 0.019 310.1
GaTe (mp-542812) <1 0 1> <0 1 0> 0.029 293.6
MgO (mp-1265) <1 1 0> <0 0 1> 0.032 127.9
InP (mp-20351) <1 0 0> <0 0 1> 0.037 106.6
C (mp-66) <1 0 0> <0 0 1> 0.037 63.9
SiC (mp-8062) <1 1 1> <1 0 0> 0.044 132.9
SiC (mp-7631) <0 0 1> <1 0 0> 0.044 132.9
SiC (mp-11714) <0 0 1> <1 0 0> 0.045 132.9
Te2Mo (mp-602) <1 0 1> <1 0 0> 0.045 221.5
LaAlO3 (mp-2920) <0 0 1> <1 0 0> 0.049 177.2
ZnO (mp-2133) <0 0 1> <1 0 0> 0.070 177.2
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.077 277.1
TbScO3 (mp-31119) <0 0 1> <0 1 0> 0.080 220.2
ZrO2 (mp-2858) <1 1 1> <0 0 1> 0.084 255.8
DyScO3 (mp-31120) <0 0 1> <0 1 0> 0.092 220.2
ZnO (mp-2133) <1 1 0> <0 0 1> 0.099 362.3
BaF2 (mp-1029) <1 1 0> <1 0 0> 0.106 221.5
SiC (mp-7631) <1 0 1> <0 0 1> 0.111 191.8
LaF3 (mp-905) <1 1 0> <0 0 1> 0.117 277.1
Mg (mp-153) <1 0 1> <0 0 1> 0.156 149.2
TeO2 (mp-2125) <1 1 0> <0 1 0> 0.157 293.6
AlN (mp-661) <1 0 0> <0 1 0> 0.158 220.2
PbSe (mp-2201) <1 1 0> <1 0 0> 0.162 221.5
Mg (mp-153) <0 0 1> <1 0 -1> 0.172 228.4
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.172 310.1
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.177 277.1
MoS2 (mp-1434) <0 0 1> <1 0 -1> 0.185 228.4
WS2 (mp-224) <0 0 1> <1 0 -1> 0.185 228.4
CdWO4 (mp-19387) <1 0 1> <0 1 0> 0.187 220.2
ZrO2 (mp-2858) <0 1 0> <1 0 0> 0.198 221.5
InAs (mp-20305) <1 0 0> <1 0 0> 0.201 310.1
SiC (mp-11714) <1 1 1> <1 0 -1> 0.214 274.1
GaSb (mp-1156) <1 1 0> <1 0 0> 0.218 221.5
GdScO3 (mp-5690) <0 0 1> <0 1 0> 0.258 220.2
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.259 191.8
PbS (mp-21276) <1 0 0> <0 0 1> 0.271 106.6
CdSe (mp-2691) <1 1 0> <1 0 0> 0.272 221.5
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.283 177.2
InP (mp-20351) <1 1 0> <0 0 1> 0.285 149.2
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.291 277.1
Al2O3 (mp-1143) <0 0 1> <1 0 0> 0.299 177.2
InSb (mp-20012) <1 1 1> <1 0 0> 0.300 310.1
SiC (mp-7631) <1 0 0> <0 0 1> 0.319 277.1
Ni (mp-23) <1 1 0> <1 0 1> 0.322 52.4
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.323 310.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
349 116 110 0 0 0
116 259 146 0 -4 0
110 146 282 0 6 0
0 0 0 99 0 -3
0 -4 6 0 102 0
0 0 0 -3 0 86
Compliance Tensor Sij (10-12Pa-1)
3.5 -1.1 -0.8 0 0 0
-1.1 5.8 -2.6 0 0.4 0
-0.8 -2.6 5.2 0 -0.4 0
0 0 0 10.1 0 0.4
0 0.4 -0.4 0 9.8 0
0 0 0 0.4 0 11.6
Shear Modulus GV
92 GPa
Bulk Modulus KV
181 GPa
Shear Modulus GR
88 GPa
Bulk Modulus KR
180 GPa
Shear Modulus GVRH
90 GPa
Bulk Modulus KVRH
181 GPa
Elastic Anisotropy
0.24
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nb9As7Pd (mp-29939) 0.7035 0.025 3
YbCrSb3 (mp-19829) 0.7077 0.049 3
LaCrSb3 (mp-19861) 0.6376 0.024 3
Sc5(NiTe)2 (mp-29769) 0.7161 0.000 3
Tb4Zn5Ge6 (mp-567401) 0.7200 0.067 3
Dy2Sb5 (mp-13451) 0.6285 0.005 2
Si5Ir3 (mp-2084) 0.5475 0.000 2
Ho2Sb5 (mp-11140) 0.6187 0.005 2
Si4Ir3 (mp-15656) 0.4394 0.000 2
Si4Rh3 (mp-540791) 0.3853 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Si Rh_pv
Final Energy/Atom
-7.0190 eV
Corrected Energy
-126.3426 eV
-126.3426 eV = -126.3426 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 24355
  • 52066
Submitted by
User remarks:
  • Rhodium silicide (4/5)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)