Material Details

Final Magnetic Moment
-0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.654 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.05 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
F43m [216]
Hall
F 4 2 3
Point Group
43m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.000 70.4
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.001 81.3
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.001 281.7
Au (mp-81) <1 1 1> <1 1 1> 0.001 211.3
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.003 211.3
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.003 172.5
MgO (mp-1265) <1 1 0> <1 1 0> 0.003 230.0
SiC (mp-8062) <1 0 0> <1 0 0> 0.003 325.3
MgO (mp-1265) <1 0 0> <1 0 0> 0.004 162.7
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.004 230.0
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.005 325.3
Al (mp-134) <1 0 0> <1 0 0> 0.005 81.3
PbS (mp-21276) <1 0 0> <1 0 0> 0.005 325.3
NaCl (mp-22862) <1 0 0> <1 0 0> 0.011 162.7
Cu (mp-30) <1 0 0> <1 0 0> 0.015 325.3
KCl (mp-23193) <1 1 1> <1 1 1> 0.017 70.4
KCl (mp-23193) <1 1 0> <1 1 0> 0.017 57.5
GaP (mp-2490) <1 1 1> <1 1 1> 0.018 211.3
GaP (mp-2490) <1 1 0> <1 1 0> 0.019 172.5
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.020 70.4
KCl (mp-23193) <1 0 0> <1 0 0> 0.020 40.7
Ag (mp-124) <1 1 1> <1 1 1> 0.024 211.3
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.024 281.7
YAlO3 (mp-3792) <1 0 1> <1 0 0> 0.043 244.0
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.064 172.5
ZnO (mp-2133) <0 0 1> <1 0 0> 0.064 325.3
GaN (mp-804) <0 0 1> <1 0 0> 0.075 284.7
CsI (mp-614603) <1 1 0> <1 1 0> 0.084 172.5
WS2 (mp-224) <0 0 1> <1 0 0> 0.090 284.7
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.090 284.7
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.098 211.3
Te2W (mp-22693) <1 0 1> <1 0 0> 0.111 203.3
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.117 325.3
Te2Mo (mp-602) <1 0 1> <1 1 1> 0.120 281.7
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.133 244.0
Ni (mp-23) <1 1 1> <1 1 1> 0.139 281.7
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.142 115.0
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.143 81.3
CdS (mp-672) <0 0 1> <1 1 0> 0.145 230.0
Mg (mp-153) <0 0 1> <1 0 0> 0.146 284.7
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.156 162.7
Mg (mp-153) <1 0 0> <1 0 0> 0.157 203.3
GaAs (mp-2534) <1 0 0> <1 0 0> 0.161 162.7
Ni (mp-23) <1 0 0> <1 0 0> 0.164 162.7
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.176 172.5
Si (mp-149) <1 1 1> <1 1 1> 0.193 211.3
Bi2Se3 (mp-541837) <0 0 1> <1 1 0> 0.195 230.0
Si (mp-149) <1 1 0> <1 1 0> 0.200 172.5
CeO2 (mp-20194) <1 1 1> <1 1 1> 0.202 211.3
InP (mp-20351) <1 0 0> <1 0 0> 0.204 325.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
150 29 29 0 0 -0
29 150 29 0 0 -0
29 29 150 0 0 -0
0 0 0 21 -0 0
0 0 0 -0 21 0
-0 -0 -0 0 0 21
Compliance Tensor Sij (10-12Pa-1)
7.1 -1.1 -1.1 0 0 0
-1.1 7.1 -1.1 0 0 0
-1.1 -1.1 7.1 0 0 0
0 0 0 46.7 0 0
0 0 0 0 46.7 0
0 0 0 0 0 46.7
Shear Modulus GV
37 GPa
Bulk Modulus KV
69 GPa
Shear Modulus GR
29 GPa
Bulk Modulus KR
69 GPa
Shear Modulus GVRH
33 GPa
Bulk Modulus KVRH
69 GPa
Elastic Anisotropy
1.42
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
BiO2 (mp-32548) 0.0000 0.101 2
CeH2 (mp-505569) 0.0000 0.000 2
BaCl2 (mp-568662) 0.0000 0.000 2
EuF2 (mp-504731) 0.0000 0.000 2
HfO2 (mp-550893) 0.0000 0.089 2
ZrFeSe (mp-961651) 0.0000 0.270 3
TiGaRh (mp-567679) 0.0000 0.552 3
ZrNiSn (mp-924129) 0.0000 0.000 3
TiBiRh (mp-961722) 0.0000 0.467 3
LiZnP (mp-569685) 0.0000 0.448 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Yb_2 Ni_pv Sb
Final Energy/Atom
-4.4667 eV
Corrected Energy
-13.4002 eV
-13.4002 eV = -13.4002 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 105332
Submitted by
User remarks:
  • High pressure experimental phase
  • Nickel antimony ytterbium (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)