Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.310 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.290 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63 [173] |
HallP 6c |
Point Group6 |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 1> | <1 0 0> | 131.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 262.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 294.3 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 113.6 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 227.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 65.6 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 196.7 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 294.3 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 327.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 262.3 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 196.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 294.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 327.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 294.3 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 327.8 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 327.8 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 294.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 196.7 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 327.8 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 118.0 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 262.3 |
Fe3O4 (mp-19306) | <1 1 1> | <1 0 0> | 131.1 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 131.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 327.8 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 65.6 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 327.8 |
Mg (mp-153) | <1 1 0> | <1 0 1> | 118.0 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 294.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 227.1 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 131.1 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 327.8 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 262.3 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 262.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 327.8 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 294.3 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 262.3 |
Fe3O4 (mp-19306) | <1 0 0> | <1 1 0> | 227.1 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 327.8 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 65.6 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 262.3 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 294.3 |
PbSe (mp-2201) | <1 0 0> | <1 1 0> | 113.6 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 327.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 327.8 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 262.3 |
C (mp-66) | <1 1 0> | <1 0 0> | 327.8 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 327.8 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 0> | 327.8 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 327.8 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 262.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tl4SnS4 (mp-5818) | 0.6687 | 0.000 | 3 |
U3Cu2S7 (mp-619067) | 0.4072 | 0.000 | 3 |
Ti(TlS)4 (mp-540939) | 0.6653 | 0.000 | 3 |
Ti(TlSe)4 (mp-540940) | 0.6462 | 0.000 | 3 |
U3Cu2Se7 (mp-541587) | 0.4226 | 0.000 | 3 |
Gd3CuGeSe7 (mp-568189) | 0.1012 | 0.000 | 4 |
Sm3CuGeSe7 (mp-570226) | 0.0629 | 0.000 | 4 |
Ce3CuGeSe7 (mp-570564) | 0.0745 | 0.000 | 4 |
La3CuGeSe7 (mp-510011) | 0.0977 | 0.000 | 4 |
Pr3CuGeSe7 (mp-571347) | 0.0363 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 Cu_pv Ge_d Se |
Final Energy/Atom-5.2674 eV |
Corrected Energy-133.0265 eV
Uncorrected energy = -126.4185 eV
Composition-based energy adjustment (-0.472 eV/atom x 14.0 atoms) = -6.6080 eV
Corrected energy = -133.0265 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)