Final Magnetic Moment0.503 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.330 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaAs + La |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI43d [220] |
HallI 4bd 2c 3 |
Point Group43m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 120.2 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 254.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 170.0 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 120.2 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 240.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 85.0 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 120.2 |
BN (mp-984) | <0 0 1> | <1 1 1> | 147.2 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 85.0 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 120.2 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 254.9 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 254.9 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 240.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 85.0 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 85.0 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 120.2 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 0> | 240.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 170.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 254.9 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 254.9 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 240.4 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 254.9 |
LiTaO3 (mp-3666) | <1 1 1> | <1 0 0> | 254.9 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 170.0 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 240.4 |
MgF2 (mp-1249) | <1 1 1> | <1 1 0> | 120.2 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 85.0 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 254.9 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 170.0 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 170.0 |
Si (mp-149) | <1 1 1> | <1 0 0> | 254.9 |
C (mp-48) | <0 0 1> | <1 1 1> | 147.2 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 0> | 120.2 |
YAlO3 (mp-3792) | <0 1 1> | <1 1 0> | 240.4 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 254.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nd(SmSb)3 (mp-675554) | 0.1088 | 0.039 | 3 |
Yb(DyS2)2 (mp-676154) | 0.1636 | 0.009 | 3 |
Yb(YS2)2 (mp-675293) | 0.1388 | 0.016 | 3 |
Tb2YbS4 (mp-673682) | 0.1582 | 0.007 | 3 |
Sm(DyS2)2 (mp-34987) | 0.1712 | 0.070 | 3 |
La4Pb3 (mp-571336) | 0.0253 | 0.000 | 2 |
Ti4P3 (mp-567920) | 0.0519 | 0.003 | 2 |
Hf3N4 (mp-11660) | 0.0524 | 0.069 | 2 |
Zr3N4 (mp-11661) | 0.0136 | 0.045 | 2 |
Eu4As3 (mp-20995) | 0.0134 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La As |
Final Energy/Atom-6.1475 eV |
Corrected Energy-86.0652 eV
-86.0652 eV = -86.0652 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)