Final Magnetic Moment
-0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.317 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.19 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
C2/m [12]
Hall
-C 2y
Point Group
2/m
Crystal System
monoclinic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
PbS (mp-21276) <1 1 1> <0 0 1> 0.004 187.0
Mg (mp-153) <0 0 1> <0 0 1> 0.004 140.2
PbS (mp-21276) <1 0 0> <1 0 -1> 0.005 179.9
LiGaO2 (mp-5854) <1 1 0> <1 0 0> 0.012 145.1
PbSe (mp-2201) <1 1 1> <1 0 0> 0.013 269.5
C (mp-48) <1 1 1> <1 0 -1> 0.018 134.9
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.018 140.2
WS2 (mp-224) <0 0 1> <0 0 1> 0.019 140.2
GaSe (mp-1943) <1 0 0> <1 0 0> 0.019 269.5
YAlO3 (mp-3792) <1 1 0> <1 0 -1> 0.019 224.9
GaSb (mp-1156) <1 1 1> <1 0 0> 0.022 269.5
LaAlO3 (mp-2920) <0 0 1> <1 0 0> 0.024 331.7
MgO (mp-1265) <1 0 0> <1 0 -1> 0.027 90.0
MoS2 (mp-1434) <1 1 0> <0 0 1> 0.031 233.7
CdSe (mp-2691) <1 1 1> <1 0 0> 0.034 269.5
TiO2 (mp-390) <1 1 1> <1 1 -1> 0.034 272.2
Mg (mp-153) <1 0 0> <1 0 -1> 0.047 134.9
Cu (mp-30) <1 1 1> <1 0 0> 0.056 269.5
GaN (mp-804) <1 1 0> <1 1 -1> 0.059 204.2
KP(HO2)2 (mp-23959) <0 0 1> <1 0 -1> 0.060 224.9
GaN (mp-804) <1 0 0> <1 0 -1> 0.061 134.9
TbScO3 (mp-31119) <0 0 1> <1 0 -1> 0.062 314.8
YAlO3 (mp-3792) <0 1 0> <1 0 -1> 0.062 269.9
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 -1> 0.064 224.9
DyScO3 (mp-31120) <0 1 1> <1 0 -1> 0.065 269.9
KCl (mp-23193) <1 1 0> <1 0 0> 0.067 290.2
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.068 186.6
AlN (mp-661) <1 0 1> <1 0 0> 0.070 269.5
DyScO3 (mp-31120) <0 0 1> <1 0 -1> 0.074 314.8
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.081 140.2
ZrO2 (mp-2858) <1 1 1> <0 1 1> 0.083 207.7
Au (mp-81) <1 1 1> <1 1 -1> 0.087 272.2
GdScO3 (mp-5690) <1 1 1> <1 0 0> 0.088 145.1
InP (mp-20351) <1 0 0> <1 0 -1> 0.093 179.9
ZrO2 (mp-2858) <1 0 1> <0 1 0> 0.094 255.4
GdScO3 (mp-5690) <1 0 0> <1 0 0> 0.096 186.6
InP (mp-20351) <1 1 1> <0 0 1> 0.096 187.0
Te2Mo (mp-602) <1 0 0> <1 0 0> 0.097 269.5
CdS (mp-672) <0 0 1> <1 0 0> 0.104 62.2
C (mp-66) <1 1 1> <1 0 0> 0.106 269.5
Ag (mp-124) <1 1 1> <1 1 -1> 0.108 272.2
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.108 220.5
TiO2 (mp-390) <1 0 0> <1 0 0> 0.110 331.7
Mg (mp-153) <1 1 0> <1 1 -1> 0.113 204.2
TiO2 (mp-2657) <1 0 0> <0 1 0> 0.121 204.3
CaCO3 (mp-3953) <0 0 1> <1 0 0> 0.122 269.5
LiAlO2 (mp-3427) <1 0 1> <0 1 0> 0.128 255.4
MgO (mp-1265) <1 1 0> <1 0 0> 0.132 103.6
LiNbO3 (mp-3731) <1 0 1> <1 0 -1> 0.133 314.8
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.134 331.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
94 45 37 0 -7 0
45 93 31 0 6 0
37 31 139 0 -2 0
0 0 0 36 0 6
-7 6 -2 0 19 0
0 0 0 6 0 19
Compliance Tensor Sij (10-12Pa-1)
15.7 -7.4 -2.4 0 8.2 0
-7.4 15.3 -1.6 0 -8 0
-2.4 -1.6 8.2 0 0.4 0
0 0 0 29.7 0 -9.9
8.2 -8 0.4 0 57.1 0
0 0 0 -9.9 0 54.8
Shear Modulus GV
29 GPa
Bulk Modulus KV
61 GPa
Shear Modulus GR
24 GPa
Bulk Modulus KR
60 GPa
Shear Modulus GVRH
27 GPa
Bulk Modulus KVRH
61 GPa
Elastic Anisotropy
1.12
Poisson's Ratio
0.31

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
256
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Cu_pv Sn_d
Final Energy/Atom
-3.9599 eV
Corrected Energy
-19.7996 eV
-19.7996 eV = -19.7996 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 417717

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)