Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.862 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density12.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 180.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 221.0 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 316.5 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 60.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 135.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 272.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 301.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 272.9 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 271.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 135.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 286.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 110.5 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 271.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 195.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 271.3 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 271.3 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 331.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 272.9 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 195.9 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 110.5 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 226.1 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 301.4 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 271.3 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 195.9 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 226.1 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 346.6 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 150.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 241.1 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 195.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 221.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 110.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 256.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 211.0 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 271.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 195.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 241.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 110.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 361.7 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 286.3 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 361.7 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 150.7 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 260.7 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 256.2 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 211.0 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 346.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 150.7 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 105.5 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 226.1 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 209.6 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 286.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
271 | 145 | 174 | 0 | 0 | 0 |
145 | 268 | 132 | 0 | 0 | 0 |
174 | 132 | 245 | 0 | 0 | 0 |
0 | 0 | 0 | 51 | 0 | 0 |
0 | 0 | 0 | 0 | 89 | 0 |
0 | 0 | 0 | 0 | 0 | 87 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
7.5 | -2 | -4.3 | 0 | 0 | 0 |
-2 | 5.6 | -1.6 | 0 | 0 | 0 |
-4.3 | -1.6 | 8 | 0 | 0 | 0 |
0 | 0 | 0 | 19.5 | 0 | 0 |
0 | 0 | 0 | 0 | 11.2 | 0 |
0 | 0 | 0 | 0 | 0 | 11.5 |
Shear Modulus GV68 GPa |
Bulk Modulus KV187 GPa |
Shear Modulus GR62 GPa |
Bulk Modulus KR186 GPa |
Shear Modulus GVRH65 GPa |
Bulk Modulus KVRH187 GPa |
Elastic Anisotropy0.47 |
Poisson's Ratio0.34 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2TbO3 (mp-686281) | 0.7449 | 0.279 | 3 |
Na2PrO3 (mp-685712) | 0.7286 | 0.222 | 3 |
Tb2Mg3Ni2 (mp-570272) | 0.6861 | 0.000 | 3 |
ZrSb2 (mp-979) | 0.7020 | 0.000 | 2 |
ZrRh (mp-567181) | 0.1615 | 0.001 | 2 |
MgSi2 (mp-1073613) | 0.6504 | 0.259 | 2 |
HfSb2 (mp-2180) | 0.7112 | 0.000 | 2 |
Mg5Si6 (mp-1075363) | 0.7152 | 0.184 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zr_sv Ir |
Final Energy/Atom-9.5549 eV |
Corrected Energy-76.4393 eV
-76.4393 eV = -76.4393 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)