Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.036 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.138 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToInSb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmmn [59] |
HallP 2 2ab 1ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 280.0 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 81.1 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 189.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 305.3 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 200.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 133.5 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 270.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 171.7 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 160.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 133.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 95.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 316.4 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 280.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 280.0 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 216.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 209.9 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 114.8 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 189.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 209.9 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 160.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 305.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 280.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 354.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 152.6 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 280.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 316.4 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 280.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 57.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 95.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 360.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 95.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 316.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 316.4 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 210.5 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 280.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 281.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 228.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 140.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 114.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 305.3 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 189.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 175.8 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 133.0 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 200.0 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 310.4 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 133.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 95.4 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 120.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 114.5 |
Te2W (mp-22693) | <0 1 1> | <1 1 1> | 177.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SbRh (mp-20619) | 0.6274 | 0.000 | 2 |
FeS (mp-1078241) | 0.6309 | 0.229 | 2 |
ZrS (mp-7859) | 0.2118 | 0.000 | 2 |
SiNi (mp-999192) | 0.6154 | 0.047 | 2 |
MgSb (mp-1094715) | 0.4116 | 0.122 | 2 |
Si (mp-8629) | 0.2019 | 0.292 | 1 |
Si (mp-92) | 0.2243 | 0.292 | 1 |
Ge (mp-78) | 0.2336 | 0.227 | 1 |
Sr (mp-10617) | 0.2719 | 0.259 | 1 |
Sn (mp-84) | 0.2237 | 0.018 | 1 |
Explore more synthesis descriptions for materials of composition InSb.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: In_d Sb |
Final Energy/Atom-3.4047 eV |
Corrected Energy-13.6187 eV
-13.6187 eV = -13.6187 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)