Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.097 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.015 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAgI + Se |
Band Gap1.590 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmna [53] |
Hall-P 2ac 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 126.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 84.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 336.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 294.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 126.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 84.2 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 262.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 87.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 210.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 131.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 84.2 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 262.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 131.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 336.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 131.1 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 126.3 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 262.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 84.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 336.8 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 153.6 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 336.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 252.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 294.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 294.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 210.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 294.7 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 153.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 336.8 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 168.4 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 153.6 |
YVO4 (mp-19133) | <1 1 1> | <1 0 1> | 262.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 252.6 |
BN (mp-984) | <0 0 1> | <0 1 1> | 87.6 |
BN (mp-984) | <1 1 1> | <0 1 1> | 262.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 230.3 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 210.5 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 294.7 |
BN (mp-984) | <1 0 0> | <0 1 0> | 76.8 |
BN (mp-984) | <1 1 0> | <0 1 1> | 262.7 |
Al (mp-134) | <1 0 0> | <1 0 1> | 131.1 |
Al (mp-134) | <1 1 0> | <0 0 1> | 252.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 124.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 168.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 42.1 |
TeO2 (mp-2125) | <1 1 1> | <0 0 1> | 210.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 84.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 210.5 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 294.7 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 248.4 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 210.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CuSe3Br (mp-28741) | 0.5095 | 0.026 | 3 |
AgTe3I (mp-570431) | 0.3328 | 0.018 | 3 |
CuSe2Cl (mp-31038) | 0.5593 | 0.000 | 3 |
CuSe3I (mp-29450) | 0.5304 | 0.000 | 3 |
CuSe2Br (mp-29567) | 0.5591 | 0.000 | 3 |
Cu3P8(S2Cl)3 (mp-559558) | 0.7081 | 0.000 | 4 |
CuP4S3I (mp-554724) | 0.4995 | 0.000 | 4 |
TlCuPSe3 (mp-569129) | 0.6649 | 0.000 | 4 |
GaAg(PSe3)2 (mp-654129) | 0.5969 | 0.000 | 4 |
SrFe2Se2O (mp-1095252) | 0.7372 | 0.000 | 4 |
Ga7Te10 (mp-18388) | 0.7173 | 0.000 | 2 |
GeS2 (mp-542613) | 0.7352 | 0.000 | 2 |
Ge4Se9 (mp-680333) | 0.7358 | 0.027 | 2 |
In7Te10 (mp-669311) | 0.6894 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ag Se I |
Final Energy/Atom-3.0661 eV |
Corrected Energy-61.3228 eV
-61.3228 eV = -61.3228 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)