Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.319 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 333.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 111.1 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 253.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 259.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 148.1 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 131.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 185.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 259.2 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 253.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 333.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 75.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 148.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 296.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 296.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 185.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 185.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 227.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 131.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 259.2 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 131.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 185.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 131.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 136.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 111.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 111.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 259.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 185.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 111.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 296.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 296.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 333.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 259.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 151.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 37.0 |
GaSe (mp-1943) | <1 1 0> | <1 0 0> | 227.4 |
GaSe (mp-1943) | <1 1 1> | <1 0 0> | 227.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 148.1 |
BN (mp-984) | <1 1 0> | <0 0 1> | 259.2 |
BN (mp-984) | <1 1 1> | <1 0 0> | 303.2 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 227.4 |
Al (mp-134) | <1 0 0> | <1 1 0> | 131.3 |
Al (mp-134) | <1 1 0> | <1 1 1> | 136.4 |
Al (mp-134) | <1 1 1> | <0 0 1> | 111.1 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 168.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 148.1 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 222.2 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 303.2 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 131.3 |
TeO2 (mp-2125) | <1 0 0> | <1 1 1> | 136.4 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 259.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2CuP (mp-675589) | 0.3398 | 0.020 | 3 |
Li2CuP (mp-12029) | 0.4281 | 0.000 | 3 |
ZrAlPt2 (mp-10906) | 0.1305 | 0.677 | 3 |
Li2CuAs (mp-15686) | 0.3677 | 0.000 | 3 |
HfAlPt2 (mp-1078728) | 0.1559 | 0.696 | 3 |
K3Sb (mp-14017) | 0.0358 | 0.000 | 2 |
Na3Sb (mp-7956) | 0.0348 | 0.000 | 2 |
Na3Bi (mp-27838) | 0.0398 | 0.000 | 2 |
K3Bi (mp-569940) | 0.0110 | 0.000 | 2 |
Rb3Sb (mp-16319) | 0.0381 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Bi |
Final Energy/Atom-2.0271 eV |
Corrected Energy-16.2164 eV
-16.2164 eV = -16.2164 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)