Final Magnetic Moment0.098 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-0.779 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4mm [107] |
HallI 4 2 |
Point Group4mm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 201.3 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 143.8 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 248.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 86.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 172.6 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 234.1 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 82.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 28.8 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 82.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 258.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 258.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 165.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 86.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 316.4 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 87.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 316.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 57.5 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 316.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 82.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 143.8 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 82.8 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 172.6 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 86.3 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 241.1 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 287.6 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 82.8 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 230.1 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 230.1 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 82.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 248.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 86.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 258.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 248.3 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 165.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 258.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 143.8 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 316.4 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 143.8 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 172.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 143.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 345.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 143.8 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 0 0> | 165.5 |
C (mp-66) | <1 0 0> | <0 0 1> | 115.0 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 86.3 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 258.8 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 258.8 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 86.3 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 316.4 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 230.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SmAsS (mp-557569) | 0.6723 | 0.001 | 3 |
ThBiTe (mp-1019362) | 0.7190 | 0.000 | 3 |
CePS (mp-1006371) | 0.5733 | 0.000 | 3 |
CeAsS (mp-1095615) | 0.6792 | 0.038 | 3 |
CeAsS (mp-1095675) | 0.5908 | 0.000 | 3 |
PuTe2 (mp-1019107) | 0.7025 | 0.669 | 2 |
PuSe2 (mp-1018954) | 0.6960 | 0.000 | 2 |
PaSb2 (mp-1018880) | 0.6975 | 0.000 | 2 |
CeSe2 (mp-1320) | 0.6832 | 0.010 | 2 |
LaTe2 (mp-571576) | 0.6019 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U P |
Final Energy/Atom-8.1517 eV |
Corrected Energy-97.8204 eV
-97.8204 eV = -97.8204 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)