material

Ta3Au

ID:

mp-569249

DOI:

10.17188/1275000


Tags: Gold tantalum (1/3)

Material Details

Final Magnetic Moment
0.124 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.023 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.009 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
17.02 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Ta2Au + Ta
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3n [223]
Hall
-P 4n 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 58599 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.001 110.1
InSb (mp-20012) <1 0 0> <1 0 0> 0.001 220.2
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.002 247.7
GaN (mp-804) <1 1 0> <1 1 0> 0.004 116.8
CdTe (mp-406) <1 0 0> <1 0 0> 0.006 220.2
GaN (mp-804) <0 0 1> <1 1 1> 0.006 143.0
CsI (mp-614603) <1 0 0> <1 0 0> 0.009 247.7
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.011 143.0
C (mp-48) <0 0 1> <1 1 1> 0.026 47.7
YAlO3 (mp-3792) <0 1 1> <1 0 0> 0.030 192.7
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.040 27.5
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.041 350.3
Ni (mp-23) <1 1 1> <1 1 1> 0.045 190.7
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.045 38.9
AlN (mp-661) <1 1 1> <1 1 0> 0.045 311.4
Ni (mp-23) <1 1 0> <1 1 0> 0.046 155.7
Ni (mp-23) <1 0 0> <1 0 0> 0.052 110.1
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.052 233.5
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.053 27.5
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.056 247.7
Ag (mp-124) <1 0 0> <1 0 0> 0.056 137.6
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.057 165.1
SiC (mp-8062) <1 0 0> <1 0 0> 0.062 247.7
ZrO2 (mp-2858) <1 1 0> <1 1 1> 0.072 238.4
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.077 350.3
AlN (mp-661) <0 0 1> <1 1 1> 0.105 333.7
KCl (mp-23193) <1 1 0> <1 1 0> 0.109 116.8
Mg (mp-153) <1 1 0> <1 1 0> 0.124 116.8
Cu (mp-30) <1 0 0> <1 0 0> 0.135 220.2
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.158 350.3
C (mp-48) <1 0 0> <1 0 0> 0.175 247.7
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.176 333.7
C (mp-48) <1 0 1> <1 0 0> 0.179 302.7
LiTaO3 (mp-3666) <1 0 0> <1 0 0> 0.180 220.2
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.180 220.2
Au (mp-81) <1 0 0> <1 0 0> 0.187 137.6
MgO (mp-1265) <1 1 0> <1 1 0> 0.200 77.8
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.203 220.2
LiNbO3 (mp-3731) <1 0 0> <1 0 0> 0.212 220.2
WS2 (mp-224) <0 0 1> <1 1 1> 0.224 143.0
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.226 143.0
C (mp-66) <1 1 0> <1 1 0> 0.228 311.4
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.229 247.7
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.248 311.4
C (mp-66) <1 0 0> <1 0 0> 0.255 220.2
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.291 155.7
Mg (mp-153) <1 0 0> <1 0 0> 0.304 82.6
MgO (mp-1265) <1 1 1> <1 1 0> 0.312 155.7
CdS (mp-672) <0 0 1> <1 0 0> 0.341 137.6
SiO2 (mp-6930) <1 1 1> <1 1 0> 0.347 155.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
393 108 108 0 0 0
108 393 108 0 0 0
108 108 393 0 0 0
0 0 0 39 0 0
0 0 0 0 39 0
0 0 0 0 0 39
Compliance Tensor Sij (10-12Pa-1)
2.9 -0.6 -0.6 0 0 0
-0.6 2.9 -0.6 0 0 0
-0.6 -0.6 2.9 0 0 0
0 0 0 25.5 0 0
0 0 0 0 25.5 0
0 0 0 0 0 25.5
Shear Modulus GV
81 GPa
Bulk Modulus KV
203 GPa
Shear Modulus GR
55 GPa
Bulk Modulus KR
203 GPa
Shear Modulus GVRH
68 GPa
Bulk Modulus KVRH
203 GPa
Elastic Anisotropy
2.30
Poisson's Ratio
0.35

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
VGe3 (mp-672337) 0.0000 0.368 2
V3Pt (mp-2211) 0.0000 0.000 2
Nb3Sn (mp-1326) 0.0000 0.000 2
GeMo3 (mp-494) 0.0000 0.000 2
V3Fe (mp-1079399) 0.0000 0.000 2
Cs (mp-949029) 0.0000 0.047 1
F2 (mp-21848) 0.0000 -0.000 1
Rb (mp-974620) 0.0000 0.036 1
Cr (mp-17) 0.0000 0.081 1
W (mp-11334) 0.0000 0.087 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ta_pv Au
Final Energy/Atom
-9.7348 eV
Corrected Energy
-77.8781 eV
-77.8781 eV = -77.8781 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 58599
Submitted by
User remarks:
  • Gold tantalum (1/3)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)