material

Mg3Pt

ID:

mp-569265

DOI:

10.17188/1275007


Tags: Magnesium platinum (3/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.577 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.010 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.76 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Mg3Pt
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 104858 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Mg (mp-153) <0 0 1> <0 0 1> 0.000 166.7
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.004 222.3
TbScO3 (mp-31119) <1 0 0> <1 1 1> 0.006 138.8
GdScO3 (mp-5690) <1 0 0> <1 1 1> 0.007 138.8
InAs (mp-20305) <1 0 0> <1 0 1> 0.007 342.6
Al2O3 (mp-1143) <0 0 1> <1 1 0> 0.008 200.6
ZnTe (mp-2176) <1 0 0> <1 0 1> 0.011 342.6
GaN (mp-804) <0 0 1> <1 1 0> 0.012 133.7
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.017 92.6
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.019 129.7
BN (mp-984) <1 1 1> <1 0 0> 0.020 270.3
GaTe (mp-542812) <1 0 0> <1 0 0> 0.025 270.3
SiC (mp-11714) <0 0 1> <0 0 1> 0.026 74.1
DyScO3 (mp-31120) <1 0 0> <1 1 1> 0.028 138.8
SiC (mp-7631) <0 0 1> <0 0 1> 0.030 74.1
TePb (mp-19717) <1 1 1> <0 0 1> 0.032 74.1
Al (mp-134) <1 0 0> <0 0 1> 0.039 129.7
CdS (mp-672) <1 1 1> <0 0 1> 0.042 259.3
TeO2 (mp-2125) <0 0 1> <1 0 0> 0.044 193.0
Ga2O3 (mp-886) <1 0 -1> <1 0 1> 0.048 342.6
NaCl (mp-22862) <1 1 1> <0 0 1> 0.049 55.6
GdScO3 (mp-5690) <0 1 0> <1 1 0> 0.051 133.7
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.056 77.2
SiC (mp-7631) <1 0 1> <1 0 0> 0.060 193.0
SiC (mp-11714) <1 0 0> <1 0 0> 0.060 347.5
SiO2 (mp-6930) <1 1 1> <1 1 1> 0.063 208.2
WS2 (mp-224) <0 0 1> <1 1 0> 0.065 133.7
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.065 133.7
Al (mp-134) <1 1 0> <0 0 1> 0.070 92.6
BN (mp-984) <1 1 0> <1 0 0> 0.075 270.3
CdWO4 (mp-19387) <0 1 0> <1 1 0> 0.076 133.7
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.078 66.9
InP (mp-20351) <1 1 0> <1 1 0> 0.082 200.6
NaCl (mp-22862) <1 0 0> <0 0 1> 0.084 352.0
Mg (mp-153) <1 0 0> <1 0 0> 0.088 270.3
NdGaO3 (mp-3196) <1 1 1> <1 0 0> 0.089 270.3
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.091 129.7
CdSe (mp-2691) <1 0 0> <1 0 1> 0.092 342.6
KTaO3 (mp-3614) <1 1 0> <0 0 1> 0.092 92.6
Te2W (mp-22693) <0 0 1> <1 0 0> 0.103 154.4
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.105 347.5
YAlO3 (mp-3792) <1 0 1> <0 0 1> 0.105 148.2
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.111 133.7
GaN (mp-804) <1 0 0> <1 0 0> 0.116 270.3
ZrO2 (mp-2858) <0 1 0> <1 0 0> 0.117 193.0
ZnSe (mp-1190) <1 1 0> <1 1 1> 0.118 138.8
GaSb (mp-1156) <1 0 0> <1 0 1> 0.121 342.6
CdTe (mp-406) <1 1 0> <1 0 0> 0.121 308.9
CdS (mp-672) <1 0 0> <1 0 0> 0.124 115.8
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.124 270.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
111 65 37 0 0 0
65 111 37 0 0 0
37 37 135 0 0 0
0 0 0 17 0 0
0 0 0 0 17 0
0 0 0 0 0 23
Compliance Tensor Sij (10-12Pa-1)
14.1 -7.7 -1.8 0 0 0
-7.7 14.1 -1.8 0 0 0
-1.8 -1.8 8.4 0 0 0
0 0 0 57.2 0 0
0 0 0 0 57.2 0
0 0 0 0 0 43.6
Shear Modulus GV
26 GPa
Bulk Modulus KV
71 GPa
Shear Modulus GR
23 GPa
Bulk Modulus KR
71 GPa
Shear Modulus GVRH
24 GPa
Bulk Modulus KVRH
71 GPa
Elastic Anisotropy
0.78
Poisson's Ratio
0.35

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li2CuP (mp-675589) 0.4511 0.020 3
Li2CuP (mp-12029) 0.4320 0.000 3
ZrAlPt2 (mp-10906) 0.2916 0.677 3
Li2CuAs (mp-15686) 0.4220 0.000 3
HfAlPt2 (mp-1078728) 0.2703 0.695 3
Li3N (mp-2341) 0.0611 0.011 2
Mg3Ir (mp-30739) 0.0401 0.015 2
Al3Ir (mp-2294) 0.0929 0.000 2
Mg3Au (mp-1078964) 0.0555 0.021 2
Mg3Pd (mp-1079229) 0.0626 0.009 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Pt
Final Energy/Atom
-3.2924 eV
Corrected Energy
-26.3393 eV
Uncorrected energy = -26.3393 eV Corrected energy = -26.3393 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 104858
Submitted by
User remarks:
  • Magnesium platinum (3/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)