Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-0.156 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density0.81 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToB5H7 + B2H5 |
Band Gap3.697 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 245.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 194.5 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 291.8 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 97.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 291.8 |
BN (mp-984) | <1 1 1> | <0 0 1> | 245.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 245.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 245.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 245.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 245.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 291.8 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 158.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 245.1 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 258.2 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 291.8 |
Fe3O4 (mp-19306) | <1 1 1> | <1 0 -1> | 253.7 |
MgO (mp-1265) | <1 0 0> | <1 0 -1> | 253.7 |
MgO (mp-1265) | <1 1 0> | <1 0 -1> | 253.7 |
MgO (mp-1265) | <1 1 1> | <1 0 -1> | 253.7 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 194.5 |
C (mp-66) | <1 0 0> | <1 0 -1> | 253.7 |
C (mp-66) | <1 1 0> | <1 0 -1> | 253.7 |
LaF3 (mp-905) | <1 0 0> | <1 0 1> | 158.5 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 245.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 245.1 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 245.1 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 194.5 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 258.2 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 245.1 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 258.2 |
SiC (mp-11714) | <1 0 0> | <1 1 -1> | 154.3 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 -1> | 253.7 |
Au (mp-81) | <1 1 0> | <0 0 1> | 245.1 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 194.5 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 291.8 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 258.2 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 258.2 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 -1> | 253.7 |
TiO2 (mp-390) | <0 0 1> | <0 1 0> | 129.1 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 291.8 |
ZnO (mp-2133) | <0 0 1> | <1 0 0> | 291.8 |
ZnO (mp-2133) | <1 1 0> | <0 0 1> | 245.1 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 194.5 |
Cu (mp-30) | <1 1 0> | <1 0 0> | 291.8 |
Al2O3 (mp-1143) | <1 0 1> | <1 0 0> | 194.5 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 194.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2B12H26O7 (mp-699473) | 0.7325 | 0.057 | 4 |
B10H13 (mp-29292) | 0.5684 | 0.005 | 2 |
B9H11 (mp-29654) | 0.4467 | 0.000 | 2 |
B10H13 (mp-776402) | 0.4852 | 0.006 | 2 |
B4H5 (mp-27798) | 0.5841 | 0.013 | 2 |
B10H13 (mp-706664) | 0.5345 | 0.005 | 2 |
CsB9H14 (mp-27590) | 0.6278 | 0.064 | 3 |
B10H13I (mp-31003) | 0.7016 | 0.000 | 3 |
B2H4C (mp-29655) | 0.6997 | 0.154 | 3 |
B5H9N (mp-27893) | 0.7204 | 0.074 | 3 |
B5H6Br (mp-30977) | 0.5804 | 0.000 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points4 |
U Values-- |
PseudopotentialsVASP PAW: B H |
Final Energy/Atom-4.6855 eV |
Corrected Energy-449.8082 eV
-449.8082 eV = -449.8082 eV (uncorrected energy)
|