Final Magnetic Moment1.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.344 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.015 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHfNi3 + Ni |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 76.9 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 314.1 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 76.9 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 251.3 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 125.7 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 251.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 355.4 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 251.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 355.4 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 230.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 222.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 222.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 311.0 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 307.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 355.4 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 314.1 |
Al (mp-134) | <1 1 0> | <1 1 0> | 188.5 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 251.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 1> | 307.8 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 44.4 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 62.8 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 76.9 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 222.1 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 251.3 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 307.8 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 88.8 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 44.4 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 222.1 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 311.0 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 177.7 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 222.1 |
C (mp-66) | <1 0 0> | <1 0 0> | 222.1 |
C (mp-66) | <1 1 0> | <1 0 0> | 355.4 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 314.1 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 188.5 |
Mg (mp-153) | <0 0 1> | <1 1 0> | 314.1 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 251.3 |
Mg (mp-153) | <1 0 1> | <1 1 0> | 188.5 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 251.3 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 222.1 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 307.8 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 222.1 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 177.7 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 125.7 |
GaP (mp-2490) | <1 1 1> | <1 0 0> | 266.5 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 177.7 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 0> | 314.1 |
TbScO3 (mp-31119) | <1 0 0> | <1 1 0> | 188.5 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 266.5 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 222.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
270 | 118 | 118 | 0 | 0 | 0 |
118 | 270 | 118 | 0 | 0 | 0 |
118 | 118 | 270 | 0 | 0 | 0 |
0 | 0 | 0 | 93 | 0 | 0 |
0 | 0 | 0 | 0 | 93 | 0 |
0 | 0 | 0 | 0 | 0 | 93 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
5.1 | -1.5 | -1.5 | 0 | 0 | 0 |
-1.5 | 5.1 | -1.5 | 0 | 0 | 0 |
-1.5 | -1.5 | 5.1 | 0 | 0 | 0 |
0 | 0 | 0 | 10.7 | 0 | 0 |
0 | 0 | 0 | 0 | 10.7 | 0 |
0 | 0 | 0 | 0 | 0 | 10.7 |
Shear Modulus GV86 GPa |
Bulk Modulus KV169 GPa |
Shear Modulus GR85 GPa |
Bulk Modulus KR169 GPa |
Shear Modulus GVRH86 GPa |
Bulk Modulus KVRH169 GPa |
Elastic Anisotropy0.05 |
Poisson's Ratio0.28 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ErInNi4 (mp-1024983) | 0.0000 | 0.000 | 3 |
DyCdNi4 (mp-1071811) | 0.0014 | 0.000 | 3 |
ErMnNi4 (mp-1077334) | 0.0000 | 0.015 | 3 |
YMgNi4 (mp-3433) | 0.0000 | 0.000 | 3 |
ErCu4Pd (mp-1077518) | 0.0007 | 0.000 | 3 |
TmCu5 (mp-30600) | 0.0039 | 0.000 | 2 |
Be5Fe (mp-1025010) | 0.0058 | 0.014 | 2 |
LuCu5 (mp-580136) | 0.0058 | 0.000 | 2 |
CeIr5 (mp-1077075) | 0.0033 | 0.327 | 2 |
UNi5 (mp-2838) | 0.0050 | 0.000 | 2 |
Co (mp-1072089) | 0.0242 | 0.199 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Hf_pv Ni_pv |
Final Energy/Atom-6.8197 eV |
Corrected Energy-40.9181 eV
-40.9181 eV = -40.9181 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)