Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.843 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.055 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.52 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
ZrTe
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 52514 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ni (mp-23) <1 1 1> <0 0 1> 0.000 85.3
Cu (mp-30) <1 1 1> <0 0 1> 0.001 158.3
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.002 158.3
SiC (mp-8062) <1 1 1> <0 0 1> 0.017 231.4
GaP (mp-2490) <1 1 1> <0 0 1> 0.018 158.3
AlN (mp-661) <0 0 1> <0 0 1> 0.019 109.6
Ge (mp-32) <1 1 1> <0 0 1> 0.024 231.4
Al (mp-134) <1 1 1> <0 0 1> 0.024 85.3
Ag (mp-124) <1 1 0> <1 0 0> 0.029 267.9
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.031 255.8
LiGaO2 (mp-5854) <1 0 0> <1 1 1> 0.043 105.9
CdWO4 (mp-19387) <1 0 1> <1 1 0> 0.055 309.3
BN (mp-984) <0 0 1> <0 0 1> 0.068 48.7
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.068 48.7
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.068 85.3
C (mp-48) <0 0 1> <0 0 1> 0.069 36.5
GaAs (mp-2534) <1 1 1> <0 0 1> 0.073 231.4
ZrO2 (mp-2858) <1 1 1> <0 0 1> 0.077 255.8
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.078 158.3
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.078 194.9
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.097 255.8
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.102 178.6
InSb (mp-20012) <1 1 1> <0 0 1> 0.103 231.4
Fe3O4 (mp-19306) <1 0 0> <1 0 1> 0.104 289.4
Au (mp-81) <1 1 0> <1 0 0> 0.104 267.9
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.109 134.0
GdScO3 (mp-5690) <1 1 0> <1 1 0> 0.109 257.8
CsI (mp-614603) <1 0 0> <1 1 0> 0.111 309.3
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.117 231.4
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.124 97.4
CdTe (mp-406) <1 1 1> <0 0 1> 0.126 231.4
PbS (mp-21276) <1 0 0> <1 0 1> 0.129 289.4
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.134 231.4
GaN (mp-804) <1 0 1> <1 1 0> 0.134 154.7
NaCl (mp-22862) <1 0 0> <0 0 1> 0.153 255.8
SrTiO3 (mp-4651) <1 0 0> <1 0 0> 0.163 89.3
DyScO3 (mp-31120) <0 1 0> <1 1 0> 0.170 257.8
GaN (mp-804) <1 0 0> <0 0 1> 0.179 134.0
BN (mp-984) <1 1 1> <0 0 1> 0.179 207.1
BaTiO3 (mp-5986) <1 1 1> <1 0 1> 0.180 257.3
TbScO3 (mp-31119) <1 1 0> <1 1 0> 0.183 257.8
LiF (mp-1138) <1 1 1> <0 0 1> 0.185 85.3
Al2O3 (mp-1143) <1 0 0> <0 0 1> 0.185 255.8
SiC (mp-7631) <0 0 1> <0 0 1> 0.188 109.6
BN (mp-984) <1 0 1> <1 0 0> 0.193 59.5
SiC (mp-11714) <0 0 1> <0 0 1> 0.201 109.6
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.203 365.4
Ni (mp-23) <1 0 0> <1 0 1> 0.207 257.3
WS2 (mp-224) <1 0 0> <0 0 1> 0.211 182.7
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.213 121.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
127 61 74 0 0 0
61 127 74 0 0 0
74 74 191 0 0 0
0 0 0 108 0 0
0 0 0 0 108 0
0 0 0 0 0 33
Compliance Tensor Sij (10-12Pa-1)
11.4 -3.7 -3 0 0 0
-3.7 11.4 -3 0 0 0
-3 -3 7.6 0 0 0
0 0 0 9.3 0 0
0 0 0 0 9.3 0
0 0 0 0 0 30.3
Shear Modulus GV
65 GPa
Bulk Modulus KV
96 GPa
Shear Modulus GR
49 GPa
Bulk Modulus KR
91 GPa
Shear Modulus GVRH
57 GPa
Bulk Modulus KVRH
93 GPa
Elastic Anisotropy
1.75
Poisson's Ratio
0.25

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Mn2SbTe (mp-675433) 0.6225 0.266 3
NaNbO2 (mp-3744) 0.5969 0.000 3
NaNbSe2 (mp-7939) 0.6216 0.000 3
LiNbSe2 (mp-1025496) 0.5959 0.000 3
Ca3SiBr2 (mp-567974) 0.5540 0.276 3
TiTe (mp-599) 0.0074 0.335 2
TcB (mp-999120) 0.1364 0.163 2
ReN (mp-999266) 0.0004 0.374 2
ZrTe (mp-1319) 0.1781 0.273 2
NiBi (mp-22861) 0.1068 0.303 2
Na (mp-999501) 0.6423 0.114 1
Xe (mp-979286) 0.5926 0.006 1
N2 (mp-1061298) 0.6134 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Te
Final Energy/Atom
-6.6880 eV
Corrected Energy
-27.5962 eV
Uncorrected energy = -26.7522 eV Composition-based energy adjustment (-0.422 eV/atom x 2.0 atoms) = -0.8440 eV Corrected energy = -27.5962 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 653214
  • 52514
  • 104197
  • 657483
  • 653230
Submitted by
User remarks:
  • Zirconium telluride (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)