material

AlAu2

ID:

mp-569558

DOI:

10.17188/1275153


Tags: Aluminum gold (1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.317 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
13.67 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 57496 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Plane
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ni (mp-23) <1 1 1> <0 1 1> 0.002 149.3
C (mp-66) <1 1 0> <1 0 1> 0.010 199.0
TiO2 (mp-390) <0 0 1> <0 1 1> 0.010 261.3
ZnO (mp-2133) <0 0 1> <0 1 1> 0.010 37.3
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.011 180.2
AlN (mp-661) <1 1 0> <1 1 1> 0.014 218.1
WSe2 (mp-1821) <1 1 0> <0 1 1> 0.014 261.3
KTaO3 (mp-3614) <1 1 1> <0 1 1> 0.018 112.0
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.021 276.6
LiF (mp-1138) <1 0 0> <1 0 0> 0.023 249.6
KTaO3 (mp-3614) <1 0 0> <0 1 1> 0.023 261.3
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.024 202.7
CdS (mp-672) <1 1 0> <1 0 1> 0.029 199.0
CaCO3 (mp-3953) <1 0 0> <0 1 1> 0.032 261.3
ZrO2 (mp-2858) <0 1 1> <1 0 0> 0.033 312.0
GaN (mp-804) <1 1 0> <1 1 1> 0.034 145.4
SiC (mp-11714) <0 0 1> <0 1 0> 0.040 148.9
SiC (mp-7631) <0 0 1> <0 1 0> 0.043 148.9
ZnSe (mp-1190) <1 1 0> <0 1 1> 0.047 186.7
NaCl (mp-22862) <1 0 0> <0 1 1> 0.049 261.3
SiC (mp-8062) <1 1 1> <0 1 0> 0.051 297.7
GaAs (mp-2534) <1 1 0> <0 1 1> 0.055 186.7
Al (mp-134) <1 1 1> <0 1 1> 0.056 112.0
NdGaO3 (mp-3196) <0 1 1> <1 0 1> 0.058 265.4
InP (mp-20351) <1 1 0> <1 0 1> 0.064 199.0
DyScO3 (mp-31120) <0 0 1> <0 1 1> 0.069 186.7
ZnSe (mp-1190) <1 0 0> <0 1 1> 0.078 261.3
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.080 90.1
LiTaO3 (mp-3666) <0 0 1> <1 0 0> 0.085 187.2
Au (mp-81) <1 1 0> <1 0 1> 0.090 199.0
Ge (mp-32) <1 1 0> <0 1 1> 0.090 186.7
BN (mp-984) <0 0 1> <0 1 1> 0.097 149.3
C (mp-66) <1 0 0> <0 0 1> 0.100 202.7
PbSe (mp-2201) <1 1 0> <0 1 0> 0.104 327.5
BN (mp-984) <1 0 1> <0 0 1> 0.106 180.2
TbScO3 (mp-31119) <1 0 1> <0 1 1> 0.107 112.0
WSe2 (mp-1821) <1 0 1> <0 0 1> 0.108 202.7
YAlO3 (mp-3792) <1 0 1> <0 1 0> 0.114 148.9
InAs (mp-20305) <1 1 1> <0 1 1> 0.115 261.3
WSe2 (mp-1821) <1 0 0> <0 1 0> 0.116 148.9
DyScO3 (mp-31120) <1 0 1> <0 1 1> 0.119 112.0
GaAs (mp-2534) <1 0 0> <0 1 1> 0.121 261.3
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.122 112.6
LiGaO2 (mp-5854) <1 0 0> <0 1 0> 0.127 178.6
Al2O3 (mp-1143) <1 0 1> <0 1 0> 0.131 268.0
ZnTe (mp-2176) <1 1 1> <0 1 1> 0.135 261.3
LiNbO3 (mp-3731) <0 0 1> <1 0 0> 0.136 187.2
LiTaO3 (mp-3666) <1 1 0> <1 0 0> 0.143 124.8
SiC (mp-11714) <1 0 1> <0 0 1> 0.144 225.2
GaN (mp-804) <1 0 1> <0 0 1> 0.147 135.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
170 88 94 0 0 0
88 196 103 0 0 0
94 103 140 0 0 0
0 0 0 34 0 0
0 0 0 0 22 0
0 0 0 0 0 38
Compliance Tensor Sij (10-12Pa-1)
9.6 -1.5 -5.3 0 0 0
-1.5 8.6 -5.3 0 0 0
-5.3 -5.3 14.6 0 0 0
0 0 0 29.2 0 0
0 0 0 0 45.2 0
0 0 0 0 0 26.4
Shear Modulus GV
34 GPa
Bulk Modulus KV
119 GPa
Shear Modulus GR
31 GPa
Bulk Modulus KR
117 GPa
Shear Modulus GVRH
32 GPa
Bulk Modulus KVRH
118 GPa
Elastic Anisotropy
0.41
Poisson's Ratio
0.37

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NdInPd (mp-642019) 0.4945 0.251 3
TiGaNi (mp-30656) 0.4826 0.000 3
ZrGaRh (mp-1078756) 0.4792 0.000 3
HfGaRh (mp-1079842) 0.5083 0.000 3
MgGaAu (mp-1080605) 0.4759 0.000 3
AlAu2 (mp-30550) 0.6191 0.004 2
MgSi (mp-1073745) 0.5666 0.207 2
MgSi (mp-1073720) 0.6155 0.237 2
MgSi (mp-1073780) 0.5800 0.148 2
Zr3Rh5 (mp-2626) 0.5870 0.000 2
Rb (mp-640416) 0.6727 0.057 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Al Au
Final Energy/Atom
-3.7477 eV
Corrected Energy
-44.9730 eV
-44.9730 eV = -44.9730 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 57496
Submitted by
User remarks:
  • Aluminum gold (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)