Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.085 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.108 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 178.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 178.0 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 197.1 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 178.0 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 178.0 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 178.0 |
Si (mp-149) | <1 0 0> | <1 0 0> | 178.0 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 -1> | 197.1 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 -1> | 197.1 |
SrTiO3 (mp-4651) | <1 0 0> | <1 0 0> | 178.0 |
Cu (mp-30) | <1 0 0> | <1 0 -1> | 197.1 |
GaTe (mp-542812) | <1 0 0> | <1 0 0> | 178.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Pt(SCl4)2 (mp-28721) | 0.6061 | 0.000 | 3 |
Al(HO)3 (mp-626605) | 0.6041 | 0.042 | 3 |
Al(HO)3 (mp-625739) | 0.6219 | 0.040 | 3 |
NaNbCl6 (mp-28178) | 0.6149 | 0.000 | 3 |
NaTaCl6 (mp-28179) | 0.6319 | 0.000 | 3 |
VN2(Cl3O)2 (mp-631589) | 0.6228 | 0.115 | 4 |
NbSeOF7 (mp-17921) | 0.6784 | 0.000 | 4 |
MnH8(N2Cl)2 (mp-696616) | 0.7439 | 0.140 | 4 |
SbXeO2F7 (mp-557823) | 0.6629 | 0.232 | 4 |
SeBr4 (mp-651332) | 0.3714 | 0.000 | 2 |
TeI4 (mp-567914) | 0.2513 | 0.007 | 2 |
SeCl4 (mp-540675) | 0.1415 | 0.000 | 2 |
SeCl4 (mp-667320) | 0.3164 | 0.014 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Cl |
Final Energy/Atom-2.7163 eV |
Corrected Energy-128.2992 eV
Uncorrected energy = -108.6512 eV
Composition-based energy adjustment (-0.614 eV/atom x 32.0 atoms) = -19.6480 eV
Corrected energy = -128.2992 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)