Final Magnetic Moment0.127 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.132 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3c [167] |
Hall-R 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 275.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 275.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 275.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 275.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 275.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 275.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 275.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 91.7 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 275.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 275.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 275.0 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 91.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 275.0 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 183.3 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 275.0 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 275.0 |
Au (mp-81) | <1 1 1> | <0 0 1> | 91.7 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 275.0 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 275.0 |
C (mp-48) | <0 0 1> | <0 0 1> | 275.0 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 275.0 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 275.0 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 275.0 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 275.0 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 91.7 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 275.0 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 91.7 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 275.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sm4Si3Pd4 (mp-680578) | 0.7236 | 0.024 | 3 |
K6Tl2Sb3 (mp-30149) | 0.6784 | 0.000 | 3 |
Tb2ZnNi2 (mp-13535) | 0.7219 | 0.000 | 3 |
Na2BiAu (mp-1078709) | 0.7130 | 0.000 | 3 |
Mg3Ga7Co2 (mp-571626) | 0.7130 | 0.000 | 3 |
Mg4Si3 (mp-1074532) | 0.6700 | 0.152 | 2 |
Rb8In11 (mp-640712) | 0.3202 | 0.000 | 2 |
Rb8Tl11 (mp-542781) | 0.1912 | 0.000 | 2 |
K8In11 (mp-582929) | 0.2375 | 0.000 | 2 |
SmAu6 (mp-1091) | 0.6842 | 0.011 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Tl_d |
Final Energy/Atom-1.9673 eV |
Corrected Energy-74.7576 eV
-74.7576 eV = -74.7576 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)