Final Magnetic Moment0.099 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.107 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <1 0 0> | <1 1 0> | 168.8 |
C (mp-48) | <1 0 1> | <1 0 0> | 223.7 |
C (mp-48) | <1 1 0> | <1 1 0> | 168.8 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 25.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 147.7 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 74.6 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 1> | 129.2 |
C (mp-48) | <0 0 1> | <1 0 0> | 134.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 29.8 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 42.2 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 168.8 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 335.9 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 189.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 63.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 189.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 223.7 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 283.4 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 337.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 189.9 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 180.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 189.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 223.7 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 74.6 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 189.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 268.5 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 295.3 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 0> | 313.2 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 134.2 |
CdWO4 (mp-19387) | <1 0 1> | <1 1 1> | 310.0 |
TePb (mp-19717) | <1 0 0> | <1 1 1> | 129.2 |
C (mp-48) | <1 1 1> | <1 1 0> | 295.3 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 126.6 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 25.8 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 232.0 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 105.5 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 84.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 223.7 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 253.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 134.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 189.9 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 180.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 74.6 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 84.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 193.9 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 168.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 253.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 105.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 134.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 74.6 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 168.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
51 | 32 | 32 | 0 | 0 | 0 |
32 | 51 | 32 | 0 | 0 | 0 |
32 | 32 | 51 | 0 | 0 | 0 |
0 | 0 | 0 | 40 | 0 | 0 |
0 | 0 | 0 | 0 | 40 | 0 |
0 | 0 | 0 | 0 | 0 | 40 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
37.9 | -14.6 | -14.6 | 0 | 0 | 0 |
-14.6 | 37.9 | -14.6 | 0 | 0 | 0 |
-14.6 | -14.6 | 37.9 | 0 | 0 | 0 |
0 | 0 | 0 | 24.8 | 0 | 0 |
0 | 0 | 0 | 0 | 24.8 | 0 |
0 | 0 | 0 | 0 | 0 | 24.8 |
Shear Modulus GV28 GPa |
Bulk Modulus KV38 GPa |
Shear Modulus GR18 GPa |
Bulk Modulus KR38 GPa |
Shear Modulus GVRH23 GPa |
Bulk Modulus KVRH38 GPa |
Elastic Anisotropy2.96 |
Poisson's Ratio0.25 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HoTmZn2 (mp-983126) | 0.0000 | 0.000 | 3 |
Pm2PtAu (mp-982772) | 0.0000 | 0.000 | 3 |
Nd2IrAu (mp-973606) | 0.0000 | 0.063 | 3 |
YbPrPd2 (mp-981530) | 0.0000 | 0.007 | 3 |
YTmAl2 (mp-980662) | 0.0000 | 0.016 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
VFeCoSb (mp-1066862) | 0.0000 | 0.164 | 4 |
ErPd (mp-851) | 0.0000 | 0.000 | 2 |
YbRu (mp-567116) | 0.0000 | 0.228 | 2 |
PrIn (mp-20023) | 0.0000 | 0.000 | 2 |
ReC (mp-1009731) | 0.0000 | 1.115 | 2 |
ScCu (mp-1169) | 0.0000 | 0.000 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.340 | 1 |
U (mp-108) | 0.0000 | 0.271 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pm_3 Mg_pv |
Final Energy/Atom-3.2806 eV |
Corrected Energy-6.5612 eV
-6.5612 eV = -6.5612 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)