material

V2NiSe4

ID:

mp-569662

DOI:

10.17188/1275199


Material Details

Final Magnetic Moment
0.060 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.477 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.128 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.00 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
V5Se8 + Ni3Se2 + VSe2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
C2/m [12]
Hall
-C 2y
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-8062) <1 1 1> <0 0 1> 0.002 66.5
SiC (mp-7631) <0 0 1> <0 0 1> 0.003 66.5
InP (mp-20351) <1 0 0> <1 0 0> 0.004 213.5
SiC (mp-11714) <0 0 1> <0 0 1> 0.004 66.5
ZnO (mp-2133) <0 0 1> <0 0 1> 0.008 177.3
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.008 288.1
GaN (mp-804) <0 0 1> <1 0 1> 0.010 242.8
NdGaO3 (mp-3196) <0 0 1> <0 1 1> 0.013 153.8
NdGaO3 (mp-3196) <1 1 0> <0 1 1> 0.016 307.5
GaN (mp-804) <1 1 1> <0 1 1> 0.017 153.8
SrTiO3 (mp-4651) <1 0 0> <0 1 0> 0.019 220.8
Fe2O3 (mp-24972) <0 0 1> <0 1 1> 0.021 230.6
Bi2Te3 (mp-34202) <0 0 1> <0 1 0> 0.022 294.5
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.022 199.5
InP (mp-20351) <1 1 0> <1 0 0> 0.023 298.9
PbSe (mp-2201) <1 0 0> <0 0 1> 0.025 155.1
GdScO3 (mp-5690) <1 0 1> <1 0 1> 0.026 340.0
GaSb (mp-1156) <1 0 0> <0 0 1> 0.027 155.1
C (mp-48) <0 0 1> <0 0 1> 0.028 133.0
BN (mp-984) <1 0 1> <1 0 0> 0.029 298.9
Au (mp-81) <1 1 0> <0 0 1> 0.030 221.6
CdWO4 (mp-19387) <1 1 0> <0 0 1> 0.031 243.8
Cu (mp-30) <1 1 0> <0 0 1> 0.031 110.8
CdSe (mp-2691) <1 0 0> <0 0 1> 0.031 155.1
CsI (mp-614603) <1 0 0> <0 1 1> 0.033 307.5
Ga2O3 (mp-886) <1 1 0> <1 0 0> 0.035 298.9
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.037 22.2
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.038 155.1
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.041 298.9
Ag (mp-124) <1 1 0> <0 0 1> 0.042 221.6
TbScO3 (mp-31119) <1 0 1> <1 0 1> 0.042 340.0
TiO2 (mp-390) <1 0 1> <0 0 1> 0.045 199.5
ZnO (mp-2133) <1 0 0> <0 1 0> 0.048 294.5
Al2O3 (mp-1143) <1 0 1> <1 0 1> 0.049 194.3
Fe2O3 (mp-24972) <1 1 0> <1 0 1> 0.049 242.8
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.053 256.2
C (mp-66) <1 0 0> <0 0 1> 0.053 88.7
SrTiO3 (mp-4651) <1 1 0> <0 1 1> 0.053 307.5
CdTe (mp-406) <1 1 0> <0 0 1> 0.053 310.3
GaN (mp-804) <1 0 1> <0 0 1> 0.054 133.0
Cu (mp-30) <1 1 1> <0 1 1> 0.055 230.6
InSb (mp-20012) <1 1 0> <0 0 1> 0.056 310.3
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.058 110.8
LiGaO2 (mp-5854) <0 1 0> <0 1 0> 0.062 294.5
SiC (mp-8062) <1 0 0> <0 0 1> 0.063 155.1
DyScO3 (mp-31120) <1 0 1> <1 0 1> 0.064 340.0
LaAlO3 (mp-2920) <1 0 0> <1 0 1> 0.066 145.7
Te2Mo (mp-602) <1 0 0> <0 0 1> 0.069 110.8
LaF3 (mp-905) <1 0 0> <0 0 1> 0.070 266.0
MgF2 (mp-1249) <1 1 1> <1 0 1> 0.080 242.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
19 7 6 0 -3 0
7 76 37 0 -3 0
6 37 78 0 -1 0
0 0 0 19 0 -1
-3 -3 -1 0 5 0
0 0 0 -1 0 7
Compliance Tensor Sij (10-12Pa-1)
58.2 -3.1 -2.7 0 25.8 0
-3.1 17.7 -8.2 0 6.7 0
-2.7 -8.2 17 0 -2.2 0
0 0 0 52.5 0 9.6
25.8 6.7 -2.2 0 201.9 0
0 0 0 9.6 0 140.9
Shear Modulus GV
15 GPa
Bulk Modulus KV
30 GPa
Shear Modulus GR
9 GPa
Bulk Modulus KR
15 GPa
Shear Modulus GVRH
12 GPa
Bulk Modulus KVRH
23 GPa
Elastic Anisotropy
3.79
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nb4IrSe10 (mp-675326) 0.6555 0.040 3
Nb15IrS32 (mp-675380) 0.6910 0.042 3
Fe3S4 (mp-7096) 0.4977 0.219 2
Tl2S (mp-667) 0.6741 0.001 2
Cr3Te4 (mp-570122) 0.3921 0.545 2
Fe3Se4 (mp-569240) 0.3628 0.173 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: V_pv Ni_pv Se
Final Energy/Atom
-5.8962 eV
Corrected Energy
-41.2737 eV
-41.2737 eV = -41.2737 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by