Final Magnetic Moment3.355 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.207 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.020 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCe3Ga + CeGa + Ce2Br5 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 291.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 109.1 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 257.3 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 308.7 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 205.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 145.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 291.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 327.4 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 63.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 181.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 218.3 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 308.7 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 145.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 109.1 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 315.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 254.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 327.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 327.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 36.4 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 51.5 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 63.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 291.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 145.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 205.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 252.1 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 181.9 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 257.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 145.5 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 205.8 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 252.1 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 315.1 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 189.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 181.9 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 257.3 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 291.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 109.1 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 181.9 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 181.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 291.1 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 254.7 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 181.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 291.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 109.1 |
BN (mp-984) | <1 0 1> | <1 0 0> | 218.3 |
BN (mp-984) | <1 1 0> | <1 1 0> | 257.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 181.9 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 254.7 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 181.9 |
Al (mp-134) | <1 0 0> | <1 0 0> | 145.5 |
Al (mp-134) | <1 1 0> | <1 1 0> | 205.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
134 | 32 | 32 | 0 | 0 | 0 |
32 | 134 | 32 | 0 | 0 | 0 |
32 | 32 | 134 | 0 | 0 | 0 |
0 | 0 | 0 | 13 | 0 | 0 |
0 | 0 | 0 | 0 | 13 | 0 |
0 | 0 | 0 | 0 | 0 | 13 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
8.2 | -1.6 | -1.6 | 0 | 0 | 0 |
-1.6 | 8.3 | -1.6 | 0 | 0 | 0 |
-1.6 | -1.6 | 8.3 | 0 | 0 | 0 |
0 | 0 | 0 | 78.6 | 0 | 0 |
0 | 0 | 0 | 0 | 78.5 | 0 |
0 | 0 | 0 | 0 | 0 | 78.6 |
Shear Modulus GV28 GPa |
Bulk Modulus KV66 GPa |
Shear Modulus GR18 GPa |
Bulk Modulus KR66 GPa |
Shear Modulus GVRH23 GPa |
Bulk Modulus KVRH66 GPa |
Elastic Anisotropy2.68 |
Poisson's Ratio0.34 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca3PCl3 (mp-29342) | 0.0000 | 0.000 | 3 |
La3GaBr3 (mp-30207) | 0.0000 | 0.000 | 3 |
Ca3AsBr3 (mp-27294) | 0.0000 | 0.000 | 3 |
Ca3AsCl3 (mp-28069) | 0.0000 | 0.000 | 3 |
Mg3NF3 (mp-7604) | 0.0000 | 0.000 | 3 |
U4S3 (mp-21063) | 0.0000 | 0.297 | 2 |
Ta4C3 (mp-1025192) | 0.0000 | 0.134 | 2 |
Cr3N4 (mp-1014460) | 0.0000 | 0.275 | 2 |
Nb4C3 (mp-15660) | 0.0000 | 0.167 | 2 |
W3N4 (mp-8102) | 0.0000 | 0.365 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce Ga_d Br |
Final Energy/Atom-4.8838 eV |
Corrected Energy-34.1865 eV
-34.1865 eV = -34.1865 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)