material

Al6Fe

ID:

mp-570001

DOI:

10.17188/1275410


Tags: Iron aluminide (1/6)

Material Details

Final Magnetic Moment
0.009 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.196 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.003 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.43 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Al13Fe4 + Al
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmcm [63]
Hall
-C 2c 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 607497 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaN (mp-804) <1 1 1> <1 0 1> 0.007 243.6
GaN (mp-804) <0 0 1> <0 0 1> 0.013 143.9
C (mp-48) <0 0 1> <0 0 1> 0.017 335.7
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.029 48.0
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.029 327.6
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.034 327.6
CdWO4 (mp-19387) <1 1 0> <1 0 0> 0.038 327.6
Au (mp-81) <1 0 0> <1 0 0> 0.041 262.1
C (mp-48) <1 0 1> <0 0 1> 0.054 239.8
NdGaO3 (mp-3196) <0 0 1> <1 0 1> 0.061 243.6
KTaO3 (mp-3614) <1 1 0> <1 1 1> 0.067 297.5
Mg (mp-153) <1 1 1> <1 0 1> 0.082 243.6
Ag (mp-124) <1 0 0> <1 0 0> 0.086 262.1
Al (mp-134) <1 1 0> <1 1 1> 0.094 297.5
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.095 327.6
CaF2 (mp-2741) <1 0 0> <1 0 1> 0.097 243.6
GaN (mp-804) <1 0 0> <0 1 0> 0.100 170.7
NdGaO3 (mp-3196) <1 1 0> <1 0 1> 0.109 243.6
GaP (mp-2490) <1 0 0> <1 0 1> 0.111 243.6
YAlO3 (mp-3792) <1 0 0> <1 0 1> 0.123 81.2
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.141 335.7
SiC (mp-11714) <1 0 1> <0 1 0> 0.142 227.6
Ni (mp-23) <1 0 0> <1 0 1> 0.145 243.6
CdS (mp-672) <1 1 1> <1 1 0> 0.150 260.4
BN (mp-984) <1 1 0> <0 1 1> 0.159 297.7
BN (mp-984) <0 0 1> <1 0 0> 0.171 65.5
LiGaO2 (mp-5854) <0 1 1> <0 1 1> 0.183 297.7
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.185 191.8
KCl (mp-23193) <1 0 0> <0 1 0> 0.186 284.6
SiC (mp-7631) <0 0 1> <0 1 0> 0.187 284.6
SiC (mp-11714) <0 0 1> <0 1 0> 0.192 284.6
CsI (mp-614603) <1 0 0> <1 0 1> 0.194 243.6
C (mp-48) <1 1 0> <0 1 1> 0.198 297.7
BaTiO3 (mp-5986) <1 0 1> <1 1 1> 0.215 297.5
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.215 287.8
TiO2 (mp-390) <1 1 0> <1 1 0> 0.217 260.4
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.245 239.8
WSe2 (mp-1821) <1 1 0> <1 0 0> 0.257 262.1
AlN (mp-661) <1 1 0> <1 1 1> 0.258 297.5
SrTiO3 (mp-4651) <0 0 1> <1 0 1> 0.259 243.6
Ni (mp-23) <1 1 0> <0 0 1> 0.284 239.8
TePb (mp-19717) <1 0 0> <0 1 0> 0.289 170.7
Mg (mp-153) <1 0 0> <0 1 0> 0.295 170.7
Si (mp-149) <1 0 0> <1 0 1> 0.296 243.6
CeO2 (mp-20194) <1 0 0> <1 0 1> 0.306 243.6
Te2W (mp-22693) <1 0 0> <0 1 1> 0.312 297.7
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.316 143.9
SiO2 (mp-6930) <0 0 1> <1 1 0> 0.317 86.8
TePb (mp-19717) <1 1 0> <0 0 1> 0.322 239.8
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.327 131.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
224 63 49 0 0 0
63 161 80 0 0 0
49 80 189 0 0 0
0 0 0 64 0 0
0 0 0 0 63 0
0 0 0 0 0 35
Compliance Tensor Sij (10-12Pa-1)
5.1 -1.7 -0.6 0 0 0
-1.7 8.4 -3.1 0 0 0
-0.6 -3.1 6.8 0 0 0
0 0 0 15.6 0 0
0 0 0 0 15.9 0
0 0 0 0 0 28.3
Shear Modulus GV
58 GPa
Bulk Modulus KV
106 GPa
Shear Modulus GR
53 GPa
Bulk Modulus KR
106 GPa
Shear Modulus GVRH
56 GPa
Bulk Modulus KVRH
106 GPa
Elastic Anisotropy
0.46
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Th2Hg (mp-30723) 0.5653 0.000 2
Al6Ru (mp-16529) 0.1622 0.000 2
Al6Re (mp-16528) 0.1733 0.006 2
Al6Tc (mp-16718) 0.1517 0.009 2
MnAl6 (mp-173) 0.1178 0.000 2
Cs (mp-573579) 0.6367 0.054 1
K (mp-573691) 0.6675 0.032 1
Bi (mp-1078637) 0.6284 0.101 1
Si (mp-1079649) 0.6485 0.428 1
Ge (mp-1079020) 0.5840 0.314 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Al Fe_pv
Final Energy/Atom
-4.6163 eV
Corrected Energy
-64.6288 eV
Uncorrected energy = -64.6288 eV Corrected energy = -64.6288 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 607497
Submitted by
User remarks:
  • Iron aluminide (1/6)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)