Final Magnetic Moment0.016 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.345 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.545 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr5Te8 + Cr |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [164] |
Hall-P 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 224.2 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 126.1 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 224.2 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 56.1 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 182.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 182.2 |
C (mp-66) | <1 1 1> | <0 0 1> | 266.3 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 266.3 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 168.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 168.2 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 266.3 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 266.3 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 88.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 266.3 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 266.3 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 112.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 168.2 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 51.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 98.1 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 168.2 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 182.2 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 126.1 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 266.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 182.2 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 176.9 |
Cu (mp-30) | <1 1 0> | <1 0 1> | 317.8 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 265.4 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 336.3 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 126.1 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 126.1 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 182.2 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 182.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 168.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 252.2 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 224.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 140.1 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 224.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 224.2 |
Al2O3 (mp-1143) | <1 0 0> | <1 0 1> | 317.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 70.1 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 98.1 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 182.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 112.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 266.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 294.3 |
TiO2 (mp-390) | <1 1 1> | <0 0 1> | 322.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 266.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 294.3 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 266.3 |
Al2O3 (mp-1143) | <1 0 1> | <0 0 1> | 336.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
77 | 26 | 16 | -2 | 0 | 0 |
26 | 77 | 16 | 2 | 0 | 0 |
16 | 16 | 30 | 0 | 0 | 0 |
-2 | 2 | 0 | 11 | 0 | 0 |
0 | 0 | 0 | 0 | 11 | -2 |
0 | 0 | 0 | 0 | -2 | 25 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
15.8 | -4.2 | -6.1 | 3.4 | 0 | 0 |
-4.2 | 15.8 | -6.1 | -3.4 | 0 | 0 |
-6.1 | -6.1 | 39.5 | 0 | 0 | 0 |
3.4 | -3.4 | 0 | 93.8 | 0 | 0 |
0 | 0 | 0 | 0 | 93.8 | 6.8 |
0 | 0 | 0 | 0 | 6.8 | 40.1 |
Shear Modulus GV18 GPa |
Bulk Modulus KV33 GPa |
Shear Modulus GR15 GPa |
Bulk Modulus KR26 GPa |
Shear Modulus GVRH16 GPa |
Bulk Modulus KVRH30 GPa |
Elastic Anisotropy1.38 |
Poisson's Ratio0.27 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cr_pv Te |
Final Energy/Atom-5.5879 eV |
Corrected Energy-39.1152 eV
-39.1152 eV = -39.1152 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)