Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.400 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHg3TeBr4 + Te2Br + TeBr4 |
Band Gap1.877 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 126.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 253.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 242.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 242.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 212.4 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 212.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 242.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 161.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 106.2 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 212.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 242.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 242.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 242.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 242.4 |
BN (mp-984) | <1 1 1> | <0 1 0> | 242.2 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 242.2 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 253.4 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 242.4 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 126.7 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 161.6 |
Au (mp-81) | <1 1 1> | <0 0 1> | 242.4 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 0> | 253.4 |
Al (mp-134) | <1 0 0> | <1 0 -1> | 212.4 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 -1> | 106.2 |
CdTe (mp-406) | <1 0 0> | <1 0 -1> | 212.4 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 0> | 126.7 |
TiO2 (mp-390) | <0 0 1> | <0 1 0> | 161.5 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 126.7 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 253.4 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 242.4 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 242.4 |
C (mp-66) | <1 0 0> | <0 1 0> | 242.2 |
Cu (mp-30) | <1 1 0> | <1 0 1> | 184.0 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 242.4 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 242.4 |
Ni (mp-23) | <1 0 0> | <1 0 1> | 184.0 |
Fe2O3 (mp-24972) | <0 0 1> | <1 0 1> | 184.0 |
InSb (mp-20012) | <1 0 0> | <1 0 -1> | 212.4 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 161.6 |
Si (mp-149) | <1 0 0> | <0 0 1> | 242.4 |
C (mp-48) | <0 0 1> | <0 0 1> | 242.4 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 1> | 184.0 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 242.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sb2S2O (mp-28711) | 0.6433 | 0.002 | 3 |
NaSO2 (mp-27500) | 0.6247 | 0.120 | 3 |
Tl2Te2O5 (mp-29690) | 0.6052 | 0.000 | 3 |
Ce(SbSe2)2 (mp-1080285) | 0.6492 | 0.299 | 3 |
Cs(SbS2)2 (mp-8890) | 0.6131 | 0.000 | 3 |
CaTiSiO5 (mp-704836) | 0.7112 | 1.072 | 4 |
SnHg2(SBr)2 (mp-554096) | 0.7233 | 0.047 | 4 |
Cd2TeCl2O3 (mp-950214) | 0.7238 | 0.005 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Hg Te Br |
Final Energy/Atom-1.8393 eV |
Corrected Energy-44.1438 eV
-44.1438 eV = -44.1438 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)