material

Bi2Pd

ID:

mp-570197

DOI:

10.17188/1275576


Tags: Urvantsevite Palladium bismuth (1/2) - HT

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.213 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.026 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
11.39 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Bi2Pd
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 56280 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.000 153.0
InAs (mp-20305) <1 0 0> <0 0 1> 0.000 153.0
Ge(Bi3O5)4 (mp-23352) <1 0 0> <0 0 1> 0.001 105.9
GaN (mp-804) <0 0 1> <0 0 1> 0.016 188.3
GdScO3 (mp-5690) <1 0 1> <0 0 1> 0.017 282.4
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.021 153.0
AlN (mp-661) <1 0 1> <1 0 1> 0.021 230.5
BN (mp-984) <1 1 0> <0 0 1> 0.023 235.3
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.035 294.1
Si (mp-149) <1 1 0> <0 0 1> 0.039 294.1
ZnO (mp-2133) <1 1 1> <0 0 1> 0.043 317.7
CdS (mp-672) <1 1 1> <1 0 0> 0.044 312.0
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.045 294.1
Mg (mp-153) <1 1 0> <0 0 1> 0.047 317.7
TeO2 (mp-2125) <1 0 1> <1 0 1> 0.047 230.5
CdS (mp-672) <0 0 1> <0 0 1> 0.048 247.1
Al2O3 (mp-1143) <1 0 0> <1 1 0> 0.048 63.0
CdSe (mp-2691) <1 0 0> <0 0 1> 0.050 153.0
Al2O3 (mp-1143) <1 0 1> <0 0 1> 0.054 200.0
LiF (mp-1138) <1 1 1> <0 0 1> 0.057 258.8
BaTiO3 (mp-5986) <1 1 1> <0 0 1> 0.059 258.8
ZrO2 (mp-2858) <1 0 0> <1 0 1> 0.060 230.5
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.061 247.1
AlN (mp-661) <1 1 1> <0 0 1> 0.064 258.8
C (mp-66) <1 1 0> <0 0 1> 0.065 200.0
GaSb (mp-1156) <1 0 0> <0 0 1> 0.073 153.0
CdS (mp-672) <1 1 0> <0 0 1> 0.075 353.0
GaAs (mp-2534) <1 0 0> <0 0 1> 0.076 294.1
TbScO3 (mp-31119) <1 0 1> <0 0 1> 0.077 282.4
Cu (mp-30) <1 0 0> <0 0 1> 0.080 105.9
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.097 105.9
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.097 247.1
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.098 258.8
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.106 282.4
ZnO (mp-2133) <1 1 0> <0 0 1> 0.107 270.6
PbSe (mp-2201) <1 0 0> <0 0 1> 0.109 153.0
GdScO3 (mp-5690) <0 1 1> <1 0 1> 0.110 276.6
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.119 176.5
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.126 133.7
TiO2 (mp-390) <0 0 1> <0 0 1> 0.126 58.8
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.137 247.1
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.140 176.5
C (mp-48) <1 0 0> <0 0 1> 0.140 153.0
Ge (mp-32) <1 0 0> <0 0 1> 0.146 294.1
InP (mp-20351) <1 1 0> <0 0 1> 0.148 247.1
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.148 58.8
DyScO3 (mp-31120) <1 0 1> <0 0 1> 0.148 282.4
CaCO3 (mp-3953) <1 0 0> <0 0 1> 0.149 176.5
C (mp-48) <0 0 1> <1 1 0> 0.149 63.0
BN (mp-984) <1 0 0> <0 0 1> 0.152 58.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
86 54 41 0 0 0
54 86 41 0 0 0
41 41 63 0 0 0
0 0 0 10 0 0
0 0 0 0 10 0
0 0 0 0 0 18
Compliance Tensor Sij (10-12Pa-1)
21.6 -9.9 -7.7 0 0 0
-9.9 21.6 -7.7 0 0 0
-7.7 -7.7 26.2 0 0 0
0 0 0 100.8 0 0
0 0 0 0 100.8 0
0 0 0 0 0 54.5
Shear Modulus GV
14 GPa
Bulk Modulus KV
57 GPa
Shear Modulus GR
13 GPa
Bulk Modulus KR
54 GPa
Shear Modulus GVRH
14 GPa
Bulk Modulus KVRH
55 GPa
Elastic Anisotropy
0.47
Poisson's Ratio
0.39

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Er2Mg3Ru (mp-1018684) 0.6728 0.015 3
Er2Mg2Ru (mp-1070135) 0.6220 0.000 3
SrZnBi2 (mp-29623) 0.7428 0.025 3
EuMnBi2 (mp-1078314) 0.7390 0.183 3
LaI2 (mp-23194) 0.4817 0.000 2
NdI2 (mp-28753) 0.4808 0.000 2
BePd2 (mp-13452) 0.2074 0.000 2
BeAu2 (mp-12761) 0.2891 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Bi Pd
Final Energy/Atom
-4.5335 eV
Corrected Energy
-13.6004 eV
Uncorrected energy = -13.6004 eV Corrected energy = -13.6004 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 56280
Submitted by
User remarks:
  • Urvantsevite
  • Palladium bismuth (1/2) - HT

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)