Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.284 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmmm [65] |
Hall-C 2 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 172.3 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 301.5 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 0> | 244.0 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 100.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 157.9 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 233.7 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 258.4 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 186.6 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 166.8 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 215.3 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 215.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 229.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 330.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 153.1 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 172.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 229.7 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 113.2 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 287.1 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 272.8 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 229.7 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 229.7 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 272.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 229.7 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 114.8 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 244.0 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 157.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 306.3 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 186.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 114.8 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 301.5 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 229.7 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 153.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 157.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 157.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 229.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 315.8 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 358.9 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 186.6 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 272.8 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 215.3 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 330.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 272.8 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 229.7 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 186.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 166.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 114.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 272.8 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 153.1 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 229.7 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 301.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
76 | 73 | 7 | 0 | 0 | 0 |
73 | 80 | 56 | 0 | 0 | 0 |
7 | 56 | -13 | 0 | 0 | 0 |
0 | 0 | 0 | 20 | 0 | 0 |
0 | 0 | 0 | 0 | 35 | 0 |
0 | 0 | 0 | 0 | 0 | 44 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
21.3 | -6.9 | -17.7 | 0 | 0 | 0 |
-6.9 | 5.3 | 19 | 0 | 0 | 0 |
-17.7 | 19 | -4.3 | 0 | 0 | 0 |
0 | 0 | 0 | 49.9 | 0 | 0 |
0 | 0 | 0 | 0 | 28.5 | 0 |
0 | 0 | 0 | 0 | 0 | 22.7 |
Shear Modulus GV20 GPa |
Bulk Modulus KV46 GPa |
Shear Modulus GR36 GPa |
Bulk Modulus KR89 GPa |
Shear Modulus GVRH28 GPa |
Bulk Modulus KVRH67 GPa |
Elastic Anisotropy-2.67 |
Poisson's Ratio0.32 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2TbO3 (mp-686281) | 0.5945 | 0.279 | 3 |
NaHo2F7 (mp-676779) | 0.6289 | 0.158 | 3 |
Tl5(Cu7Se5)2 (mp-28656) | 0.7077 | 0.019 | 3 |
KBi2F7 (mp-675634) | 0.6994 | 0.069 | 3 |
RbMg6Mo (mp-1100163) | 0.6699 | 0.523 | 3 |
Li13Si4 (mp-672287) | 0.6586 | 0.000 | 2 |
K4Pb9 (mp-680443) | 0.5938 | 0.007 | 2 |
Dy3Ge4 (mp-612918) | 0.6485 | 0.005 | 2 |
Rb4Pb9 (mp-680463) | 0.6110 | 0.000 | 2 |
Y3Ge4 (mp-17381) | 0.6565 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 Mg_pv Ni_pv |
Final Energy/Atom-3.9456 eV |
Corrected Energy-27.6192 eV
-27.6192 eV = -27.6192 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)