material

AgBr

ID:

mp-570301

DOI:

10.17188/1275629


Tags: High pressure experimental phase Silver bromide - II, HP

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.326 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.042 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.25 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
AgBr
Band Gap
0.760 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21/m [11]
Hall
-P 2yb
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 56549 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
No elastic tensor calculated for this material, so elastic energies not avaialable. Sorting by MCIA instead.
substrate material substrate orientation film orientation MCIA [Å2]
LaAlO3 (mp-2920) <1 0 1> <1 0 1> 239.8
AlN (mp-661) <0 0 1> <1 0 1> 59.9
CeO2 (mp-20194) <1 0 0> <0 0 1> 153.8
GaAs (mp-2534) <1 1 0> <1 0 0> 48.6
GaAs (mp-2534) <1 1 1> <1 0 1> 59.9
BaF2 (mp-1029) <1 0 0> <0 0 1> 153.8
BaF2 (mp-1029) <1 1 0> <0 1 0> 216.3
GaN (mp-804) <0 0 1> <0 1 1> 206.4
GaN (mp-804) <1 0 0> <0 1 0> 264.4
GaN (mp-804) <1 1 0> <1 1 1> 268.9
SiO2 (mp-6930) <0 0 1> <1 1 1> 345.8
SiO2 (mp-6930) <1 1 1> <0 1 0> 216.3
DyScO3 (mp-31120) <0 1 0> <1 1 0> 136.7
DyScO3 (mp-31120) <1 0 1> <1 0 0> 170.0
InAs (mp-20305) <1 0 0> <0 0 1> 153.8
InAs (mp-20305) <1 1 0> <0 1 0> 216.3
ZnSe (mp-1190) <1 0 0> <1 1 0> 34.2
ZnSe (mp-1190) <1 1 1> <1 0 1> 59.9
KTaO3 (mp-3614) <1 0 0> <0 0 1> 17.1
KTaO3 (mp-3614) <1 1 0> <1 0 0> 24.3
KTaO3 (mp-3614) <1 1 1> <0 0 1> 85.4
CdS (mp-672) <0 0 1> <1 0 1> 30.0
CdS (mp-672) <1 0 0> <0 0 1> 85.4
CdS (mp-672) <1 0 1> <0 1 0> 168.2
CdS (mp-672) <1 1 0> <1 0 1> 149.9
CdS (mp-672) <1 1 1> <1 0 1> 209.8
LiF (mp-1138) <1 0 0> <0 0 1> 17.1
LiF (mp-1138) <1 1 0> <1 0 0> 24.3
LiF (mp-1138) <1 1 1> <0 0 1> 85.4
Te2W (mp-22693) <0 0 1> <1 1 1> 153.7
Te2W (mp-22693) <0 1 0> <0 1 0> 216.3
Te2W (mp-22693) <0 1 1> <0 0 1> 290.4
Te2W (mp-22693) <1 1 0> <0 1 0> 216.3
LaAlO3 (mp-2920) <0 0 1> <0 1 1> 176.9
LaAlO3 (mp-2920) <1 1 1> <0 0 1> 256.3
AlN (mp-661) <1 0 0> <0 1 0> 168.2
AlN (mp-661) <1 0 1> <0 1 0> 120.2
AlN (mp-661) <1 1 0> <0 1 0> 216.3
YVO4 (mp-19133) <0 0 1> <1 0 1> 209.8
YVO4 (mp-19133) <1 0 0> <1 0 1> 89.9
YVO4 (mp-19133) <1 0 1> <1 0 1> 209.8
YVO4 (mp-19133) <1 1 0> <0 0 1> 256.3
AlN (mp-661) <1 1 1> <0 1 0> 144.2
CeO2 (mp-20194) <1 1 0> <0 1 0> 264.4
TePb (mp-19717) <1 0 0> <0 0 1> 85.4
TePb (mp-19717) <1 1 0> <1 1 1> 307.4
GaAs (mp-2534) <1 0 0> <1 1 0> 34.2
Te2Mo (mp-602) <0 0 1> <1 0 1> 89.9
Te2Mo (mp-602) <1 0 0> <0 1 0> 216.3
Te2Mo (mp-602) <1 0 1> <0 1 0> 216.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
49 31 35 -0 0 0
31 54 31 -0 0 0
35 31 48 -0 0 0
-0 -0 -0 8 0 0
0 0 0 0 12 -0
0 0 0 0 -0 8
Compliance Tensor Sij (10-12Pa-1)
46.3 -12.2 -25.3 0 0 0
-12.2 32.7 -12.3 0.1 0 0
-25.3 -12.3 46.8 0.2 0 0
0 0.1 0.2 130.9 0 0
0 0 0 0 86.5 0.3
0 0 0 0 0.3 130.1
Shear Modulus GV
9 GPa
Bulk Modulus KV
38 GPa
Shear Modulus GR
9 GPa
Bulk Modulus KR
38 GPa
Shear Modulus GVRH
9 GPa
Bulk Modulus KVRH
38 GPa
Elastic Anisotropy
0.22
Poisson's Ratio
0.39

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
InCuSe2 (mp-676764) 0.2099 0.204 3
LiFe2O3 (mp-769789) 0.2234 0.094 3
InAgSe2 (mp-686712) 0.2481 0.112 3
LiInSe2 (mp-34489) 0.2318 0.115 3
Li2NbS3 (mp-754779) 0.2487 0.085 3
Li2NbVO4 (mp-771635) 0.2370 0.109 4
Li2VO2F (mp-764027) 0.2511 0.050 4
Li2VO2F (mp-777720) 0.2027 0.048 4
Li3NbV2O6 (mp-773262) 0.2330 0.091 4
Li4Ti3NbO8 (mp-756660) 0.2296 0.088 4
RbN (mp-1064529) 0.2262 1.514 2
CdTe (mp-1066480) 0.1591 0.181 2
RbN (mp-1066707) 0.1780 1.513 2
InSb (mp-21210) 0.1826 0.140 2
SrN (mp-1078609) 0.2353 0.438 2
Na6MnNi3(SbO6)2 (mp-1094109) 0.7177 0.139 5
Hg (mp-982872) 0.3406 0.020 1
Sb (mp-632286) 0.2723 0.059 1
Te (mp-570459) 0.4114 0.044 1
Te (mp-10654) 0.3938 0.047 1
Te (mp-105) 0.2321 0.047 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

The chalcogenide membrane (AgBrAg2SAs2S3HgI2) was prepared according to the procedure described elsewhere [25]. The resultant melt was air quenched and a section of the membrane was fashioned into [...]
In a typical procedure, 2mmol of Bi(NO3)35H2O, 0.2mmol AgNO3 and 3mmol 1-hexadecyl-3-methylimidazolium bromide ([C16mim]Br), 0.5g polyvinylpyrrolidone (PVP, Mw=104) were dissolved in 40mL ethyl [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition AgBr.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ag Br
Final Energy/Atom
-2.5605 eV
Corrected Energy
-11.3100 eV
Uncorrected energy = -10.2420 eV Composition-based energy adjustment (-0.534 eV/atom x 2.0 atoms) = -1.0680 eV Corrected energy = -11.3100 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 56549
Submitted by
User remarks:
  • High pressure experimental phase
  • Silver bromide - II, HP

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)