Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-0.331 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.025 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaBC + La(BC)2 + La2C3 |
Band Gap0.046 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP41212 [92] |
HallP 4abw 2nw |
Point Group422 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 150.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 301.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 301.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 75.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 301.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 150.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 226.0 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 301.4 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 75.3 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 226.0 |
C (mp-66) | <1 1 1> | <0 0 1> | 226.0 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 226.0 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 150.7 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 150.7 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 301.4 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 75.3 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 301.4 |
Si (mp-149) | <1 0 0> | <0 0 1> | 150.7 |
Au (mp-81) | <1 0 0> | <0 0 1> | 301.4 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 75.3 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 301.4 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 226.0 |
CaCO3 (mp-3953) | <1 1 0> | <0 0 1> | 150.7 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 150.7 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 75.3 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 301.4 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 75.3 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 150.7 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 301.4 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 226.0 |
Ge (mp-32) | <1 0 0> | <0 0 1> | 301.4 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 150.7 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 226.0 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 75.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlAg(WO4)2 (mvc-591) | 0.6874 | 0.187 | 4 |
AlNi(WO4)2 (mvc-613) | 0.7162 | 0.231 | 4 |
AlNi(WO4)2 (mvc-16235) | 0.7167 | 0.230 | 4 |
Rb2Nb3Cl7O5 (mp-558393) | 0.6959 | 0.000 | 4 |
K2Nb3Cl7O5 (mp-559790) | 0.6854 | 0.000 | 4 |
MoO3 (mvc-14941) | 0.7418 | 0.010 | 2 |
TiF4 (mp-28974) | 0.7195 | 0.000 | 2 |
Nb2O5 (mp-680944) | 0.7023 | 0.000 | 2 |
Nb2O5 (mp-556048) | 0.6273 | 0.010 | 2 |
Nd10(B3C4)3 (mp-571244) | 0.1523 | 0.040 | 3 |
PrBC (mp-570767) | 0.4084 | 0.000 | 3 |
Pr10(B3C4)3 (mp-567719) | 0.1053 | 0.037 | 3 |
La15B14C19 (mp-679949) | 0.4288 | 0.023 | 3 |
LaBC (mp-568090) | 0.3440 | 0.000 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points3 |
U Values-- |
PseudopotentialsVASP PAW: La B C |
Final Energy/Atom-7.4300 eV |
Corrected Energy-921.3227 eV
-921.3227 eV = -921.3227 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)