Final Magnetic Moment0.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.321 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mcm [140] |
Hall-I 4 2c |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 80.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 80.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 161.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 242.7 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 180.7 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 114.4 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 114.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 161.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 161.6 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 228.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 228.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 161.6 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 228.8 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 161.8 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 242.7 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 242.7 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 161.8 |
LaF3 (mp-905) | <0 0 1> | <1 0 1> | 180.7 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 80.9 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 114.4 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 161.6 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 242.7 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 161.6 |
WS2 (mp-224) | <1 0 0> | <1 0 1> | 180.7 |
YAlO3 (mp-3792) | <0 1 1> | <1 0 0> | 242.7 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 161.6 |
GaTe (mp-542812) | <0 0 1> | <1 1 0> | 228.8 |
LiAlO2 (mp-3427) | <1 0 0> | <1 0 0> | 161.8 |
GaTe (mp-542812) | <1 0 -1> | <1 1 0> | 228.8 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 161.8 |
LiAlO2 (mp-3427) | <1 1 0> | <1 1 0> | 228.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nb5SiSn2 (mp-7557) | 0.6525 | 0.001 | 3 |
Ti5FeSb2 (mp-30326) | 0.6402 | 0.022 | 3 |
Ti5Sb2Rh (mp-16687) | 0.5290 | 0.030 | 3 |
Ti5CuSb2 (mp-13020) | 0.5018 | 0.001 | 3 |
Nb5GaSn2 (mp-17230) | 0.6025 | 0.000 | 3 |
Ce5Sn3 (mp-637308) | 0.1922 | 0.000 | 2 |
Dy5In3 (mp-568144) | 0.2135 | 0.000 | 2 |
Pu5Ir3 (mp-2848) | 0.1619 | 0.000 | 2 |
Pr5Sn3 (mp-570696) | 0.1484 | 0.002 | 2 |
La5Sn3 (mp-510494) | 0.0885 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 Tl_d |
Final Energy/Atom-4.1943 eV |
Corrected Energy-67.1096 eV
-67.1096 eV = -67.1096 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)