Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.076 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.46 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.324 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 192.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 289.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 192.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 289.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 289.1 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 289.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 289.1 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 289.1 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 192.7 |
C (mp-66) | <1 1 0> | <0 0 1> | 289.1 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 192.7 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 192.7 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 192.7 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 289.1 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 289.1 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 192.7 |
Fe2O3 (mp-24972) | <1 0 0> | <0 0 1> | 289.1 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 192.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mo3(HO5)2 (mp-626751) | 0.7350 | 0.153 | 3 |
Ru2S4Cl13 (mp-653758) | 0.7158 | 0.067 | 3 |
RhSe2Cl7 (mp-613545) | 0.7239 | 0.004 | 3 |
TaP4(SCl)5 (mp-572763) | 0.6807 | 0.007 | 4 |
TaP4S4Cl5 (mp-555967) | 0.3671 | 0.008 | 4 |
TaP2Se2Cl5 (mp-571250) | 0.0596 | 0.000 | 4 |
TaP2S2Cl5 (mp-556728) | 0.2229 | 0.000 | 4 |
NbP2S2Cl5 (mp-679987) | 0.2729 | 0.000 | 4 |
FeO3 (mp-863847) | 0.5968 | 0.557 | 2 |
SrCd2H16(Cl3O4)2 (mp-759862) | 0.7457 | 0.062 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv P Se Cl |
Final Energy/Atom-4.4947 eV |
Corrected Energy-359.5786 eV
-359.5786 eV = -359.5786 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)