Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.460 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.030 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPNCl2 + TaCl5 |
Band Gap3.166 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 -1> | 178.1 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 206.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 182.0 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 262.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 242.8 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 242.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 242.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 242.8 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 242.8 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 242.8 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 242.8 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 242.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 242.8 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 242.8 |
Ga2O3 (mp-886) | <1 0 -1> | <0 1 1> | 262.3 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 182.0 |
Au (mp-81) | <1 1 0> | <0 0 1> | 242.8 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 -1> | 178.1 |
ZnO (mp-2133) | <1 1 0> | <1 0 0> | 182.0 |
Cu (mp-30) | <1 1 1> | <0 1 0> | 206.4 |
MoSe2 (mp-1634) | <1 1 0> | <1 0 -1> | 178.1 |
Au (mp-81) | <1 1 1> | <0 0 1> | 242.8 |
WSe2 (mp-1821) | <1 1 0> | <1 0 -1> | 178.1 |
Fe2O3 (mp-24972) | <0 0 1> | <0 1 0> | 206.4 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 0> | 182.0 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 242.8 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 242.8 |
ZnTe (mp-2176) | <1 0 0> | <0 1 1> | 262.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MoSO6 (mp-704102) | 0.6847 | 0.007 | 3 |
Re2S2O13 (mp-974650) | 0.5731 | 0.000 | 3 |
Mo2P2O11 (mp-637201) | 0.6404 | 0.016 | 3 |
VRe2O9 (mp-32532) | 0.7025 | 0.000 | 3 |
Mo2P2O11 (mp-540142) | 0.6985 | 0.000 | 3 |
MoPCl5O3 (mp-567661) | 0.5375 | 0.137 | 4 |
TiPCl7O (mp-559493) | 0.6766 | 0.000 | 4 |
KVSO6 (mp-566353) | 0.6619 | 0.000 | 4 |
MoP(Cl3O)2 (mp-566590) | 0.6733 | 0.071 | 4 |
VP2Cl7O4 (mp-647553) | 0.6245 | 0.066 | 4 |
MgC2S2(OF3)2 (mp-684804) | 0.6267 | 0.470 | 5 |
MoPN(Cl3O)2 (mp-617599) | 0.5696 | 0.185 | 5 |
MoPNCl6O (mp-649091) | 0.7007 | 0.140 | 5 |
NdH32C8N4Cl7 (mp-738618) | 0.7487 | 0.069 | 5 |
SbH32C8N4Cl7 (mp-708994) | 0.7457 | 0.066 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ta_pv P N Cl |
Final Energy/Atom-4.8603 eV |
Corrected Energy-213.0460 eV
Uncorrected energy = -194.4100 eV
Composition-based energy adjustment (-0.361 eV/atom x 4.0 atoms) = -1.4440 eV
Composition-based energy adjustment (-0.614 eV/atom x 28.0 atoms) = -17.1920 eV
Corrected energy = -213.0460 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)