material

NbCo3

ID:

mp-570557

DOI:

10.17188/1275776


Tags: Niobium cobalt (1/3) - HT

Material Details

Final Magnetic Moment
1.932 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FiM
Formation Energy / Atom
-0.093 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.066 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.00 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
NbCo3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63mc [186]
Hall
P 6c 2c
Point Group
6mm
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-11714) <0 0 1> <0 0 1> 0.007 57.9
SiC (mp-7631) <0 0 1> <0 0 1> 0.011 57.9
Ge (mp-32) <1 0 0> <0 0 1> 0.013 366.5
PbS (mp-21276) <1 1 1> <0 0 1> 0.018 250.8
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.024 77.2
Ge (mp-32) <1 1 1> <0 0 1> 0.034 57.9
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.038 73.0
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.039 289.4
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.042 270.1
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.043 292.1
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.050 253.0
Te2W (mp-22693) <1 0 0> <1 0 0> 0.059 292.1
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.070 292.1
Te2Mo (mp-602) <1 0 0> <1 0 0> 0.071 219.1
TiO2 (mp-390) <0 0 1> <1 0 1> 0.090 302.1
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.093 250.8
LaF3 (mp-905) <0 0 1> <0 0 1> 0.101 135.0
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.102 308.6
GaAs (mp-2534) <1 1 1> <0 0 1> 0.102 57.9
YVO4 (mp-19133) <1 1 1> <1 1 0> 0.106 253.0
BN (mp-984) <1 1 0> <1 0 1> 0.129 302.1
BN (mp-984) <0 0 1> <0 0 1> 0.137 135.0
InSb (mp-20012) <1 1 1> <0 0 1> 0.144 77.2
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.150 253.0
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.162 57.9
C (mp-66) <1 1 0> <0 0 1> 0.163 289.4
Au (mp-81) <1 1 1> <0 0 1> 0.167 366.5
CdTe (mp-406) <1 1 1> <0 0 1> 0.174 77.2
LiF (mp-1138) <1 0 0> <0 0 1> 0.178 135.0
Mg (mp-153) <1 0 0> <0 0 1> 0.179 250.8
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.185 77.2
Al (mp-134) <1 1 1> <0 0 1> 0.185 250.8
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.191 366.5
CdTe (mp-406) <1 1 0> <0 0 1> 0.209 308.6
ZnSe (mp-1190) <1 1 0> <0 0 1> 0.218 231.5
Te2W (mp-22693) <0 1 0> <1 0 0> 0.221 219.1
InSb (mp-20012) <1 1 0> <0 0 1> 0.228 308.6
YAlO3 (mp-3792) <0 0 1> <1 1 0> 0.234 253.0
SiC (mp-8062) <1 1 1> <0 0 1> 0.238 135.0
GaN (mp-804) <1 0 0> <0 0 1> 0.253 250.8
NaCl (mp-22862) <1 1 0> <0 0 1> 0.258 231.5
GaAs (mp-2534) <1 1 0> <0 0 1> 0.265 231.5
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.285 77.2
Mg (mp-153) <1 1 1> <0 0 1> 0.303 366.5
Ag (mp-124) <1 1 1> <0 0 1> 0.318 366.5
LiAlO2 (mp-3427) <1 0 1> <1 1 0> 0.322 126.5
WSe2 (mp-1821) <1 0 1> <1 1 0> 0.349 253.0
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.355 292.1
GaN (mp-804) <0 0 1> <0 0 1> 0.361 173.6
InP (mp-20351) <1 1 1> <0 0 1> 0.366 250.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
343 143 130 0 0 0
143 343 130 0 0 0
130 130 304 0 0 0
0 0 0 74 0 0
0 0 0 0 74 0
0 0 0 0 0 100
Compliance Tensor Sij (10-12Pa-1)
3.8 -1.2 -1.1 0 0 0
-1.2 3.8 -1.1 0 0 0
-1.1 -1.1 4.3 0 0 0
0 0 0 13.5 0 0
0 0 0 0 13.5 0
0 0 0 0 0 10
Shear Modulus GV
89 GPa
Bulk Modulus KV
199 GPa
Shear Modulus GR
87 GPa
Bulk Modulus KR
198 GPa
Shear Modulus GVRH
88 GPa
Bulk Modulus KVRH
199 GPa
Elastic Anisotropy
0.11
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ca2Mg3Si (mp-1095343) 0.3470 0.119 3
NdMgNi4 (mp-11194) 0.3466 0.000 3
Zr2Fe3Ge (mp-21040) 0.3517 0.000 3
Zr2Fe3Si (mp-16336) 0.3431 0.000 3
Mg2Cu3Si (mp-10746) 0.3490 0.000 3
Fe2W (mp-20868) 0.3085 0.000 2
LuMn5 (mp-30770) 0.2830 0.211 2
NbFe2 (mp-937052) 0.3124 0.015 2
ZrRu2 (mp-569979) 0.3147 0.067 2
Fe2Mo (mp-1095682) 0.3070 0.002 2
Co (mp-1072089) 0.3822 0.199 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Nb_pv Co
Final Energy/Atom
-7.9499 eV
Corrected Energy
-190.7964 eV
-190.7964 eV = -190.7964 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 150944
Submitted by
User remarks:
  • Niobium cobalt (1/3) - HT

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)