Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.370 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.031 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.45 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSi3N4 + AlN + Sr2Si5N8 |
Band Gap3.582 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPna21 [33] |
HallP 2c 2n |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 176.2 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 242.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 293.7 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 242.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 176.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 293.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 211.6 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 242.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 176.2 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 234.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 293.7 |
Al (mp-134) | <1 1 0> | <0 1 0> | 211.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 211.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 176.2 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 293.7 |
Ga2O3 (mp-886) | <0 1 0> | <0 0 1> | 293.7 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 293.7 |
Ga2O3 (mp-886) | <1 1 0> | <0 0 1> | 293.7 |
Au (mp-81) | <1 1 0> | <0 0 1> | 293.7 |
Au (mp-81) | <1 1 1> | <0 1 0> | 211.6 |
C (mp-48) | <0 0 1> | <0 1 0> | 105.8 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 176.2 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 176.2 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 176.2 |
CaCO3 (mp-3953) | <1 0 1> | <0 0 1> | 176.2 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 58.7 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 176.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 293.7 |
MgAl2O4 (mp-3536) | <1 1 0> | <0 0 1> | 293.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 293.7 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 211.6 |
SrTiO3 (mp-4651) | <1 1 1> | <0 1 0> | 211.6 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 234.9 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 176.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 293.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 293.7 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 211.6 |
Ge (mp-32) | <1 1 0> | <0 0 1> | 293.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 293.7 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 293.7 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 293.7 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 293.7 |
C (mp-66) | <1 0 0> | <0 0 1> | 176.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 176.2 |
C (mp-66) | <1 1 1> | <0 0 1> | 176.2 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 0> | 211.6 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 293.7 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 293.7 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 293.7 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 0> | 211.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SrSi7N10 (mp-570598) | 0.6057 | 0.011 | 3 |
BaGe7N10 (mp-1029679) | 0.7157 | 0.000 | 3 |
BaSi7N10 (mp-29703) | 0.6530 | 0.000 | 3 |
VCuO3 (mp-614005) | 0.5983 | 0.081 | 3 |
KSi5N7 (mp-1029584) | 0.2438 | 0.000 | 3 |
Li2Fe5Si5O16 (mp-767707) | 0.6185 | 0.049 | 4 |
Li2Si5Ni5O16 (mp-761373) | 0.6337 | 0.095 | 4 |
Li2FeSi3O8 (mp-767149) | 0.6362 | 0.075 | 4 |
Li2Si3NiO8 (mp-863897) | 0.6353 | 0.093 | 4 |
Li2MnSi3O8 (mp-761653) | 0.6300 | 0.076 | 4 |
Li3BePCO7 (mp-771341) | 0.6925 | 0.051 | 5 |
SrAl2SiN2O3 (mp-554390) | 0.7305 | 0.003 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv Al Si N |
Final Energy/Atom-7.7399 eV |
Corrected Energy-804.9484 eV
-804.9484 eV = -804.9484 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)