Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.225 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.018 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density16.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToU3Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 162.9 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 281.6 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 219.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 144.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 204.8 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 219.5 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 219.5 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 90.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 144.8 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 199.1 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 181.0 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 144.8 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 204.8 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 325.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 108.6 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 125.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 307.2 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 204.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 289.6 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 179.2 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 230.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 144.8 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 219.5 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 156.8 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 230.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 271.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 162.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 281.6 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 219.5 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 90.5 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 230.4 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 219.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 162.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 230.4 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 282.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 54.3 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 282.2 |
Te2Mo (mp-602) | <1 1 0> | <1 1 0> | 281.6 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 90.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 18.1 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 25.6 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 31.4 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 179.2 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 179.2 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 128.0 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 230.4 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 153.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 125.4 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 108.6 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 307.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.034 | 3 |
LiCa6Ge (mp-12609) | 0.0000 | 0.183 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.065 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
YbTl3 (mp-570164) | 0.0000 | 0.000 | 2 |
TiRh3 (mp-1152) | 0.0000 | 0.000 | 2 |
Rb3Os (mp-1066774) | 0.0000 | 1.446 | 2 |
LaTl3 (mp-2001) | 0.0000 | 0.000 | 2 |
URu3 (mp-1263) | 0.0000 | 0.000 | 2 |
Na (mp-974558) | 0.0000 | 0.003 | 1 |
Br (mp-998870) | 0.0000 | 0.666 | 1 |
Mn (mp-8634) | 0.0000 | 0.083 | 1 |
Pb (mp-20483) | 0.0000 | 0.000 | 1 |
Cu (mp-30) | 0.0000 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U Si |
Final Energy/Atom-10.0502 eV |
Corrected Energy-40.2008 eV
-40.2008 eV = -40.2008 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)