Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.196 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.009 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiC |
Band Gap2.020 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [160] |
HallR 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 232.9 |
GaTe (mp-542812) | <0 0 1> | <0 0 1> | 291.2 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 158.1 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 33.3 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 74.9 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 274.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 8.3 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 158.1 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 187.8 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 158.1 |
C (mp-48) | <0 0 1> | <0 0 1> | 99.8 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 8.3 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 187.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 316.1 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 108.1 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 166.4 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 199.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 108.1 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 199.7 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 158.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 208.0 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 282.8 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 158.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 266.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 291.2 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 266.2 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 266.2 |
CsI (mp-614603) | <1 1 1> | <0 0 1> | 108.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 33.3 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 116.5 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 124.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 141.4 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 133.1 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 58.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 74.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 174.7 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 174.7 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 158.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 291.2 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 324.4 |
GaTe (mp-542812) | <1 0 0> | <0 0 1> | 133.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 166.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 208.0 |
BN (mp-984) | <1 1 1> | <0 0 1> | 307.8 |
Au (mp-81) | <1 1 1> | <0 0 1> | 208.0 |
ZrO2 (mp-2858) | <1 1 1> | <0 0 1> | 208.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 124.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 224.6 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 183.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 166.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
487 | 104 | 51 | -13 | 0 | 0 |
104 | 487 | 51 | 13 | 0 | 0 |
51 | 51 | 535 | 0 | 0 | 0 |
-13 | 13 | 0 | 161 | 0 | 0 |
0 | 0 | 0 | 0 | 161 | -13 |
0 | 0 | 0 | 0 | -13 | 192 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
2.2 | -0.4 | -0.2 | 0.2 | 0 | 0 |
-0.4 | 2.2 | -0.2 | -0.2 | 0 | 0 |
-0.2 | -0.2 | 1.9 | 0 | 0 | 0 |
0.2 | -0.2 | 0 | 6.2 | 0 | 0 |
0 | 0 | 0 | 0 | 6.2 | 0.4 |
0 | 0 | 0 | 0 | 0.4 | 5.2 |
Shear Modulus GV190 GPa |
Bulk Modulus KV214 GPa |
Shear Modulus GR185 GPa |
Bulk Modulus KR214 GPa |
Shear Modulus GVRH187 GPa |
Bulk Modulus KVRH214 GPa |
Elastic Anisotropy0.14 |
Poisson's Ratio0.16 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Si3NiP4 (mp-8311) | 0.1911 | 0.000 | 3 |
Cu2SiTe3 (mp-675120) | 0.1867 | 0.001 | 3 |
In2AsSe (mp-676682) | 0.1921 | 0.137 | 3 |
Li3SbS4 (mp-760415) | 0.1836 | 0.005 | 3 |
CrCd3Te4 (mp-1079533) | 0.1896 | 0.115 | 3 |
ZnCu2GeS4 (mp-6408) | 0.1669 | 0.000 | 4 |
CoCu2SiS4 (mp-11769) | 0.1788 | 0.065 | 4 |
ZnCu2SiTe4 (mp-1078498) | 0.1800 | 0.000 | 4 |
LiIn2CuSe4 (mp-1079491) | 0.1819 | 0.004 | 4 |
ZnCu2SnS4 (mp-1079541) | 0.1800 | 0.000 | 4 |
ZnS (mp-554986) | 0.0124 | 0.001 | 2 |
SiC (mp-568696) | 0.0152 | 0.001 | 2 |
ZnS (mp-556468) | 0.0152 | 0.012 | 2 |
SiC (mp-570804) | 0.0145 | 0.032 | 2 |
SiC (mp-9947) | 0.0152 | 0.009 | 2 |
C (mp-611448) | 0.0366 | 0.143 | 1 |
C (mp-616440) | 0.0312 | 0.141 | 1 |
C (mp-569517) | 0.0456 | 0.145 | 1 |
C (mp-569567) | 0.0282 | 0.144 | 1 |
Ge (mp-1091415) | 0.0749 | 0.008 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si C |
Final Energy/Atom-7.5215 eV |
Corrected Energy-120.3440 eV
Uncorrected energy = -120.3440 eV
Corrected energy = -120.3440 eV
|