Final Magnetic Moment1.977 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.702 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.086 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.34 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToWC + H4C + W6CCl18 + H4NCl + C |
Band Gap0.091 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [164] |
Hall-P 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 292.8 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 169.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 107.1 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 292.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 97.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 107.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 292.8 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 195.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 107.1 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 292.8 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 292.8 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 107.1 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 292.8 |
C (mp-48) | <0 0 1> | <1 1 0> | 169.0 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 107.1 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 292.8 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 0> | 195.2 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 292.8 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 292.8 |
CsI (mp-614603) | <1 1 1> | <0 0 1> | 107.1 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 107.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Pb3SO6 (mp-22023) | 0.7098 | 0.007 | 3 |
Tl2SO4 (mp-4112) | 0.7457 | 0.000 | 3 |
K4CO4 (mp-550547) | 0.6208 | 0.261 | 3 |
Rb4CO4 (mp-551267) | 0.6334 | 0.257 | 3 |
Rb4CO4 (mp-556527) | 0.7437 | 0.196 | 3 |
NdHSO5 (mp-23831) | 0.7430 | 0.000 | 4 |
LaCrHO5 (mp-25686) | 0.7462 | 0.000 | 4 |
FeH12C4NCl4 (mp-603940) | 0.7132 | 0.085 | 5 |
Nb3H12C4NCl9 (mp-569921) | 0.2338 | 0.067 | 5 |
CuTe4H12C4N (mp-570909) | 0.7122 | 0.095 | 5 |
HgH24C8(I2N)2 (mp-605659) | 0.7142 | 0.115 | 5 |
GaH12C4NCl3 (mp-600257) | 0.7191 | 0.080 | 5 |
KSn2H36C12(Se2N)3 (mp-708999) | 0.6908 | 0.088 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: H W_pv C N Cl |
Final Energy/Atom-5.3187 eV |
Corrected Energy-319.5339 eV
Uncorrected energy = -308.4819 eV
Composition-based energy adjustment (-0.614 eV/atom x 18.0 atoms) = -11.0520 eV
Corrected energy = -319.5339 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)