material

Ba5Al5Sn

ID:

mp-570677

DOI:

10.17188/1275850


Tags: Pentabarium pentaaluminide stannide

Material Details

Final Magnetic Moment
0.030 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.348 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.33 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P6m2 [187]
Hall
P 6 2
Point Group
6m2
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 416338 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnO (mp-2133) <0 0 1> <0 0 1> 0.000 290.3
CdS (mp-672) <0 0 1> <0 0 1> 0.003 290.3
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.006 290.3
C (mp-48) <0 0 1> <0 0 1> 0.006 225.8
NaCl (mp-22862) <1 1 1> <0 0 1> 0.012 225.8
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.013 290.3
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.018 225.8
TePb (mp-19717) <1 1 1> <0 0 1> 0.020 225.8
SiC (mp-7631) <0 0 1> <0 0 1> 0.021 225.8
GaN (mp-804) <0 0 1> <0 0 1> 0.021 225.8
Ni (mp-23) <1 0 0> <0 0 1> 0.024 258.0
SiC (mp-11714) <0 0 1> <0 0 1> 0.024 225.8
Mg (mp-153) <1 1 1> <1 0 1> 0.025 151.1
C (mp-66) <1 1 1> <0 0 1> 0.026 290.3
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.027 273.2
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.033 290.3
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.041 273.2
CdTe (mp-406) <1 1 1> <0 0 1> 0.044 225.8
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.048 225.8
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.055 225.8
InSb (mp-20012) <1 1 1> <0 0 1> 0.055 225.8
AlN (mp-661) <0 0 1> <0 0 1> 0.064 225.8
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.067 96.8
GaN (mp-804) <1 1 0> <1 1 0> 0.067 118.3
Cu (mp-30) <1 1 1> <0 0 1> 0.072 290.3
GaAs (mp-2534) <1 1 1> <0 0 1> 0.073 225.8
GaN (mp-804) <1 1 1> <1 0 1> 0.077 151.1
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.087 273.2
MgO (mp-1265) <1 1 0> <0 0 1> 0.102 129.0
Ga2O3 (mp-886) <1 0 -1> <1 0 1> 0.103 75.5
SiC (mp-7631) <1 1 0> <0 0 1> 0.111 161.3
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.117 225.8
Ge (mp-32) <1 1 1> <0 0 1> 0.125 225.8
Al (mp-134) <1 0 0> <1 0 0> 0.128 273.2
BN (mp-984) <1 0 1> <0 0 1> 0.133 225.8
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.138 32.3
Ni (mp-23) <1 1 0> <0 0 1> 0.139 258.0
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.144 161.3
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.160 258.0
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.164 204.9
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 0.169 129.0
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.173 290.3
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.184 96.8
Mg (mp-153) <1 1 0> <1 1 0> 0.185 118.3
PbS (mp-21276) <1 0 0> <0 0 1> 0.188 258.0
LiTaO3 (mp-3666) <1 0 0> <0 0 1> 0.189 290.3
WS2 (mp-224) <0 0 1> <0 0 1> 0.189 225.8
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.190 225.8
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.191 290.3
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.192 290.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
54 12 20 0 0 0
12 54 20 0 0 0
20 20 56 0 0 0
0 0 0 17 0 0
0 0 0 0 17 0
0 0 0 0 0 21
Compliance Tensor Sij (10-12Pa-1)
21.7 -2.4 -6.9 0 0 0
-2.4 21.7 -6.9 0 0 0
-6.9 -6.9 22.6 0 0 0
0 0 0 60.4 0 0
0 0 0 0 60.4 0
0 0 0 0 0 48.2
Shear Modulus GV
18 GPa
Bulk Modulus KV
30 GPa
Shear Modulus GR
18 GPa
Bulk Modulus KR
30 GPa
Shear Modulus GVRH
18 GPa
Bulk Modulus KVRH
30 GPa
Elastic Anisotropy
0.08
Poisson's Ratio
0.25

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ba5Ga5Pb (mp-605650) 0.2839 0.000 3
Ba5Al5Pb (mp-568809) 0.0539 0.000 3
Ba5Ga5Sn (mp-568967) 0.1999 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Al Sn_d
Final Energy/Atom
-3.2862 eV
Corrected Energy
-36.1483 eV
-36.1483 eV = -36.1483 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 416338
Submitted by
User remarks:
  • Pentabarium pentaaluminide stannide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)