material

Ti3Sn

ID:

mp-570691

DOI:

10.17188/1275859


Tags: Tin titanium (1/3) - HP

Material Details

Final Magnetic Moment
0.004 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.266 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.038 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.02 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Ti3Sn
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 106087 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.001 210.5
Au (mp-81) <1 0 0> <1 0 0> 0.003 17.4
Au (mp-81) <1 1 0> <1 1 0> 0.003 24.6
Au (mp-81) <1 1 1> <1 1 1> 0.003 30.1
GaP (mp-2490) <1 1 1> <1 1 1> 0.004 210.5
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.005 120.3
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.006 86.8
Ag (mp-124) <1 0 0> <1 0 0> 0.007 17.4
Ag (mp-124) <1 1 0> <1 1 0> 0.008 24.6
Ag (mp-124) <1 1 1> <1 1 1> 0.008 30.1
Bi2Se3 (mp-541837) <0 0 1> <1 0 0> 0.009 121.6
Cu (mp-30) <1 1 0> <1 1 0> 0.014 73.7
Cu (mp-30) <1 1 1> <1 1 1> 0.014 90.2
GaTe (mp-542812) <1 0 1> <1 1 0> 0.017 98.2
SiC (mp-11714) <1 0 1> <1 0 0> 0.030 260.5
TePb (mp-19717) <1 0 0> <1 0 0> 0.031 86.8
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 0> 0.036 225.7
C (mp-48) <1 0 1> <1 1 0> 0.039 319.3
PbSe (mp-2201) <1 0 0> <1 0 0> 0.039 156.3
PbSe (mp-2201) <1 1 0> <1 1 0> 0.045 221.0
TiO2 (mp-390) <1 0 0> <1 0 0> 0.045 260.5
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.045 156.3
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.048 138.9
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.052 86.8
CdS (mp-672) <0 0 1> <1 0 0> 0.057 121.6
CdS (mp-672) <1 0 0> <1 0 0> 0.058 86.8
Y3Fe5O12 (mp-19648) <1 0 0> <1 0 0> 0.059 156.3
NdGaO3 (mp-3196) <0 0 1> <1 0 0> 0.060 277.8
GaSb (mp-1156) <1 0 0> <1 0 0> 0.068 156.3
SiC (mp-11714) <1 0 0> <1 1 0> 0.068 221.0
KCl (mp-23193) <1 1 1> <1 1 1> 0.071 210.5
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.071 225.7
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.072 156.3
GaSb (mp-1156) <1 1 0> <1 1 0> 0.079 221.0
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.083 221.0
GaN (mp-804) <1 1 1> <1 0 0> 0.096 277.8
CdSe (mp-2691) <1 0 0> <1 0 0> 0.098 156.3
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.098 260.5
Te2W (mp-22693) <1 1 0> <1 1 0> 0.099 221.0
CdTe (mp-406) <1 0 0> <1 0 0> 0.100 86.8
PbS (mp-21276) <1 1 1> <1 0 0> 0.104 312.6
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.111 191.0
SiC (mp-11714) <0 0 1> <1 0 0> 0.111 173.7
CdSe (mp-2691) <1 1 0> <1 1 0> 0.113 221.0
SiC (mp-7631) <0 0 1> <1 0 0> 0.114 173.7
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.118 221.0
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.118 156.3
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.119 312.6
InSb (mp-20012) <1 0 0> <1 0 0> 0.122 86.8
Ge (mp-32) <1 1 1> <1 0 0> 0.123 173.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
129 107 107 0 0 0
107 129 107 0 0 0
107 107 129 0 0 0
0 0 0 86 0 0
0 0 0 0 86 0
0 0 0 0 0 86
Compliance Tensor Sij (10-12Pa-1)
30.4 -13.7 -13.7 0 0 0
-13.7 30.4 -13.7 0 0 0
-13.7 -13.7 30.4 0 0 0
0 0 0 11.7 0 0
0 0 0 0 11.7 0
0 0 0 0 0 11.7
Shear Modulus GV
56 GPa
Bulk Modulus KV
114 GPa
Shear Modulus GR
24 GPa
Bulk Modulus KR
114 GPa
Shear Modulus GVRH
40 GPa
Bulk Modulus KVRH
114 GPa
Elastic Anisotropy
6.82
Poisson's Ratio
0.34

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.1125 0.005 3
CrCoPt2 (mp-570863) 0.0492 0.000 3
LiCa6Ge (mp-12609) 0.0000 0.180 3
GaFeNi2 (mp-1065359) 0.0412 0.066 3
GaCo2Ni (mp-1018060) 0.0157 0.075 3
Cr8Ni50Mo15W2 (mp-767372) 0.2155 0.028 4
CrFeCoNi (mp-1012640) 0.3608 0.118 4
CrFeCoNi (mp-1096923) 0.4019 0.193 4
Be3Tc (mp-977552) 0.0000 0.000 2
AlC3 (mp-1065540) 0.0000 2.748 2
TiCo3 (mp-608) 0.0000 0.000 2
DyPt3 (mp-2465) 0.0000 0.000 2
MgCd3 (mp-1094839) 0.0000 0.015 2
Sr (mp-76) 0.0000 0.006 1
N2 (mp-1056857) 0.0000 0.000 1
Ni (mp-1056486) 0.0000 0.000 1
Cd (mp-1096861) 0.0000 0.001 1
Pd (mp-1056438) 0.0000 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Sn_d
Final Energy/Atom
-7.1855 eV
Corrected Energy
-28.7421 eV
Uncorrected energy = -28.7421 eV Corrected energy = -28.7421 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 106087
Submitted by
User remarks:
  • Tin titanium (1/3) - HP

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)