material

V3Au

ID:

mp-570698

DOI:

10.17188/1275865


Tags: Gold vanadium (1/3)

Material Details

Final Magnetic Moment
0.891 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
0.065 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.101 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.96 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
V3Au
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 58611 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ni (mp-23) <1 1 0> <1 1 0> 0.000 191.5
LiAlO2 (mp-3427) <1 0 0> <1 1 0> 0.001 297.8
LaF3 (mp-905) <0 0 1> <1 1 1> 0.006 182.4
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.007 225.6
SiO2 (mp-6930) <1 1 0> <1 1 0> 0.010 191.5
BN (mp-984) <0 0 1> <1 1 1> 0.011 104.2
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.011 234.0
ZrO2 (mp-2858) <1 1 -1> <1 1 0> 0.014 319.1
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.015 42.5
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.021 63.8
Si (mp-149) <1 0 0> <1 0 0> 0.029 30.1
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.030 255.7
Si (mp-149) <1 1 0> <1 1 0> 0.032 42.5
ZrO2 (mp-2858) <0 1 1> <1 0 0> 0.034 315.9
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.034 30.1
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.037 42.5
TiO2 (mp-2657) <1 0 1> <1 1 0> 0.042 127.6
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.045 165.5
TbScO3 (mp-31119) <1 1 1> <1 0 0> 0.048 285.8
Ge(Bi3O5)4 (mp-23352) <1 1 1> <1 1 1> 0.049 182.4
GaP (mp-2490) <1 0 0> <1 0 0> 0.051 30.1
GaP (mp-2490) <1 1 0> <1 1 0> 0.056 42.5
WS2 (mp-224) <1 1 0> <1 1 0> 0.056 234.0
Te2W (mp-22693) <0 0 1> <1 0 0> 0.057 330.9
SiC (mp-7631) <1 0 1> <1 0 0> 0.063 240.7
WS2 (mp-224) <1 0 1> <1 1 0> 0.064 276.5
CaCO3 (mp-3953) <1 1 0> <1 0 0> 0.065 150.4
GaSe (mp-1943) <1 0 0> <1 0 0> 0.070 135.4
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.083 225.6
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.089 135.4
MoSe2 (mp-1634) <1 0 0> <1 1 0> 0.092 255.3
Mg (mp-153) <1 0 0> <1 1 0> 0.094 148.9
KTaO3 (mp-3614) <1 1 1> <1 0 0> 0.094 225.6
Al (mp-134) <1 1 1> <1 0 0> 0.099 225.6
MoS2 (mp-1434) <1 1 1> <1 1 0> 0.099 234.0
Te2W (mp-22693) <0 1 0> <1 0 0> 0.108 270.8
GaSe (mp-1943) <1 0 1> <1 1 0> 0.108 276.5
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.109 30.1
Mg (mp-153) <0 0 1> <1 1 1> 0.110 26.1
WS2 (mp-224) <1 1 1> <1 1 1> 0.110 78.2
DyScO3 (mp-31120) <0 1 1> <1 1 0> 0.111 106.4
InP (mp-20351) <1 1 1> <1 1 1> 0.113 182.4
TiO2 (mp-390) <1 0 1> <1 0 0> 0.114 120.3
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.114 63.8
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.119 42.5
AlN (mp-661) <1 1 1> <1 0 0> 0.122 225.6
DyScO3 (mp-31120) <1 1 1> <1 0 0> 0.123 285.8
Bi2Te3 (mp-34202) <0 0 1> <1 1 0> 0.137 85.1
NdGaO3 (mp-3196) <0 1 1> <1 1 1> 0.139 52.1
GaSe (mp-1943) <0 0 1> <1 0 0> 0.143 75.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
199 171 171 0 0 0
171 199 171 0 0 0
171 171 199 0 0 0
0 0 0 80 0 0
0 0 0 0 80 0
0 0 0 0 0 80
Compliance Tensor Sij (10-12Pa-1)
24.8 -11.5 -11.5 0 0 0
-11.5 24.8 -11.5 0 0 0
-11.5 -11.5 24.8 0 0 0
0 0 0 12.4 0 0
0 0 0 0 12.4 0
0 0 0 0 0 12.4
Shear Modulus GV
54 GPa
Bulk Modulus KV
180 GPa
Shear Modulus GR
27 GPa
Bulk Modulus KR
180 GPa
Shear Modulus GVRH
41 GPa
Bulk Modulus KVRH
180 GPa
Elastic Anisotropy
4.80
Poisson's Ratio
0.40

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.1125 0.005 3
CrCoPt2 (mp-570863) 0.0492 0.034 3
LiCa6Ge (mp-12609) 0.0000 0.183 3
GaFeNi2 (mp-1065359) 0.0412 0.065 3
GaCo2Ni (mp-1018060) 0.0157 0.075 3
Cr8Ni50Mo15W2 (mp-767372) 0.2155 0.028 4
CrFeCoNi (mp-1012640) 0.3608 0.065 4
CrFeCoNi (mp-1096923) 0.4019 0.193 4
Ce3Ga (mp-19920) 0.0000 0.000 2
VC3 (mp-1067129) 0.0000 2.503 2
YSn3 (mp-11571) 0.0000 0.024 2
ErIn3 (mp-1291) 0.0000 0.000 2
Ti3Au (mp-11260) 0.0000 0.124 2
H2 (mp-634659) 0.0000 2.277 1
Sn (mp-1022725) 0.0000 0.054 1
Sr (mp-76) 0.0000 0.006 1
Ni (mp-1056486) 0.0000 0.000 1
Cd (mp-1096861) 0.0000 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: V_pv Au
Final Energy/Atom
-7.5668 eV
Corrected Energy
-30.2670 eV
Uncorrected energy = -30.2670 eV Corrected energy = -30.2670 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 58611
Submitted by
User remarks:
  • Gold vanadium (1/3)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)