Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.988 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.172 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToIN4 + VCl4 + VN + I |
Band Gap1.005 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 223.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 133.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 223.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 133.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 230.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 312.5 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 260.6 |
CdS (mp-672) | <1 0 1> | <1 -1 -1> | 268.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 133.9 |
Te2W (mp-22693) | <1 0 0> | <1 0 -1> | 285.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 267.9 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 208.5 |
Te2Mo (mp-602) | <1 1 1> | <1 0 -1> | 285.6 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 247.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 223.2 |
BN (mp-984) | <0 0 1> | <0 1 0> | 260.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 178.6 |
BN (mp-984) | <1 0 1> | <1 1 1> | 224.5 |
BN (mp-984) | <1 1 0> | <1 0 0> | 237.1 |
BN (mp-984) | <1 1 1> | <1 -1 1> | 68.3 |
LiNbO3 (mp-3731) | <0 0 1> | <1 -1 0> | 263.3 |
LiNbO3 (mp-3731) | <1 1 1> | <0 1 0> | 260.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 312.5 |
Bi2Se3 (mp-541837) | <1 0 1> | <0 1 -1> | 256.7 |
MoS2 (mp-1434) | <0 0 1> | <1 -1 1> | 204.8 |
MoS2 (mp-1434) | <1 0 1> | <0 1 -1> | 205.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 133.9 |
Al (mp-134) | <1 1 0> | <1 0 1> | 230.7 |
Al (mp-134) | <1 1 1> | <1 0 1> | 230.7 |
LiGaO2 (mp-5854) | <0 0 1> | <1 -1 0> | 329.1 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 -1> | 262.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 -1> | 256.7 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 -1> | 174.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 -1 1> | 136.5 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 296.3 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 223.2 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 307.6 |
TeO2 (mp-2125) | <0 0 1> | <1 1 -1> | 262.1 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 296.3 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 296.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 178.6 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 142.8 |
AlN (mp-661) | <1 0 1> | <1 -1 0> | 263.3 |
AlN (mp-661) | <1 1 0> | <1 -1 0> | 329.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 89.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 89.3 |
CeO2 (mp-20194) | <1 1 0> | <1 -1 0> | 329.1 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 153.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 133.9 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 223.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: V_pv I N Cl |
Final Energy/Atom-4.7081 eV |
Corrected Energy-61.6607 eV
Uncorrected energy = -56.4967 eV
Composition-based energy adjustment (-0.379 eV/atom x 2.0 atoms) = -0.7580 eV
Composition-based energy adjustment (-0.361 eV/atom x 2.0 atoms) = -0.7220 eV
Composition-based energy adjustment (-0.614 eV/atom x 6.0 atoms) = -3.6840 eV
Corrected energy = -61.6607 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)