Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.715 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.047 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSr8(MnN3)3 + SrMnN2 + Li7MnN4 + Mn |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 208.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 238.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 268.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 208.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 232.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 232.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 119.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 238.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 208.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 224.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 208.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 89.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 328.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 232.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 208.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 232.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 232.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 119.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 208.8 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 358.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 112.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 149.2 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 116.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 119.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 29.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 208.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 328.2 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 194.7 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 268.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 119.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 29.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 119.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 268.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 208.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 89.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 268.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 89.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 149.2 |
Al (mp-134) | <1 1 0> | <0 0 1> | 119.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 0> | 194.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 358.0 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 268.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 29.8 |
TeO2 (mp-2125) | <1 0 1> | <1 0 1> | 232.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 208.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 328.2 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 224.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 89.5 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 29.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2N2O (mp-761019) | 0.6317 | 0.096 | 3 |
AgPtO2 (mp-997007) | 0.6664 | 0.041 | 3 |
Li3FeS3 (mp-777742) | 0.6462 | 0.246 | 3 |
Na2Te2As (mp-29381) | 0.6614 | 0.009 | 3 |
Zr2N2O (mp-776250) | 0.6478 | 0.093 | 3 |
Li8Mn(O2F)2 (mp-780086) | 0.6937 | 0.071 | 4 |
Sr2Li2NiO4 (mp-769674) | 0.6532 | 0.091 | 4 |
K2Th(CuS2)2 (mp-555425) | 0.6805 | 0.013 | 4 |
Li3CaMnN3 (mp-569112) | 0.2380 | 0.027 | 4 |
ZnCuBiO5 (mvc-7505) | 0.6776 | 0.152 | 4 |
CoSb2 (mp-755) | 0.7265 | 0.002 | 2 |
Bi2Rh (mp-23217) | 0.7333 | 0.000 | 2 |
MgSi2 (mp-1073358) | 0.6762 | 0.177 | 2 |
MgSi2 (mp-1073369) | 0.7168 | 0.192 | 2 |
MgSi2 (mp-1073644) | 0.7203 | 0.163 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv Li_sv Mn_pv N |
Final Energy/Atom-5.7699 eV |
Corrected Energy-94.4844 eV
Uncorrected energy = -92.3184 eV
Composition-based energy adjustment (-0.361 eV/atom x 6.0 atoms) = -2.1660 eV
Corrected energy = -94.4844 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)