Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.684 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.095 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.29 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToK2SnSe3 + SnSe |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4cm [108] |
HallI 4 2c |
Point Group4mm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 1> | 270.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 203.7 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 251.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 67.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 237.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 271.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 270.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 251.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 67.9 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 237.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 237.2 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 270.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 271.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 296.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 237.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 271.6 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 237.2 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 251.6 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 270.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 67.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 177.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 271.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 177.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 67.9 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 296.6 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 237.2 |
BN (mp-984) | <0 0 1> | <1 1 0> | 251.6 |
BN (mp-984) | <1 1 1> | <1 0 0> | 237.2 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 237.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 271.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 296.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 1> | 90.2 |
CdTe (mp-406) | <1 1 1> | <1 0 0> | 237.2 |
C (mp-66) | <1 0 0> | <1 0 0> | 177.9 |
TeO2 (mp-2125) | <0 1 0> | <1 0 1> | 270.5 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 203.7 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 237.2 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 237.2 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 271.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 237.2 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 296.6 |
TiO2 (mp-2657) | <1 1 0> | <1 1 0> | 251.6 |
C (mp-66) | <1 1 0> | <1 0 0> | 177.9 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 177.9 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 271.6 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 296.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 67.9 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 296.6 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 1> | 90.2 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 237.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tl3In7Se10 (mp-675519) | 0.2866 | 0.034 | 3 |
NaInTe2 (mp-22483) | 0.1829 | 0.000 | 3 |
TlInSe2 (mp-568517) | 0.1581 | 0.332 | 3 |
KInTe2 (mp-19851) | 0.2568 | 0.000 | 3 |
TlInTe2 (mp-22791) | 0.2534 | 0.000 | 3 |
MnTl2SnTe4 (mp-569859) | 0.3351 | 0.000 | 4 |
Tl2CdSnTe4 (mp-570076) | 0.2401 | 0.009 | 4 |
K2CdSnSe4 (mp-1079645) | 0.3630 | 0.000 | 4 |
Rb2SnHgTe4 (mp-1080691) | 0.3641 | 0.000 | 4 |
Tl2SnHgTe4 (mp-570051) | 0.2452 | 0.012 | 4 |
TlSe (mp-1836) | 0.2005 | 0.000 | 2 |
TlS (mp-322) | 0.3254 | 0.052 | 2 |
InTe (mp-20320) | 0.2936 | 0.011 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Sn_d Se |
Final Energy/Atom-3.7078 eV |
Corrected Energy-29.6625 eV
-29.6625 eV = -29.6625 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)