material

Ti2BRh6

ID:

mp-571126

DOI:

10.17188/1276100


Tags: Dititanium hexarhodium boride

Material Details

Final Magnetic Moment
0.006 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.691 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.70 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 415337 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Au (mp-81) <1 0 0> <1 0 0> 0.000 313.2
SiC (mp-8062) <1 0 0> <1 0 0> 0.028 250.6
Ag (mp-124) <1 0 0> <1 0 0> 0.031 313.2
SiC (mp-7631) <0 0 1> <1 1 1> 0.044 108.5
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.051 62.6
Mg (mp-153) <1 0 0> <1 0 0> 0.052 250.6
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.052 88.6
SiC (mp-11714) <0 0 1> <1 1 1> 0.052 108.5
SrTiO3 (mp-4651) <1 0 1> <1 1 1> 0.069 108.5
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.077 313.2
PbSe (mp-2201) <1 0 0> <1 0 0> 0.106 313.2
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.120 62.6
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.125 250.6
CdS (mp-672) <0 0 1> <1 1 1> 0.150 108.5
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.151 62.6
GaSb (mp-1156) <1 0 0> <1 0 0> 0.167 313.2
MgF2 (mp-1249) <1 0 1> <1 1 0> 0.170 265.8
Ag (mp-124) <1 1 0> <1 1 0> 0.198 265.8
CdWO4 (mp-19387) <0 1 0> <1 1 0> 0.212 265.8
CsI (mp-614603) <1 0 0> <1 0 0> 0.222 62.6
CsI (mp-614603) <1 1 0> <1 1 0> 0.225 88.6
CdSe (mp-2691) <1 0 0> <1 0 0> 0.226 313.2
CsI (mp-614603) <1 1 1> <1 1 1> 0.227 108.5
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.269 88.6
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.270 62.6
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.297 265.8
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.300 187.9
CdS (mp-672) <1 0 0> <1 0 0> 0.303 313.2
MgO (mp-1265) <1 0 0> <1 0 0> 0.314 313.2
GaN (mp-804) <1 0 0> <1 0 0> 0.327 250.6
C (mp-48) <1 0 0> <1 0 0> 0.332 250.6
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.347 250.6
GdScO3 (mp-5690) <0 1 0> <1 1 0> 0.360 88.6
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.366 313.2
Au (mp-81) <1 1 0> <1 1 0> 0.387 265.8
WS2 (mp-224) <1 1 0> <1 0 0> 0.398 313.2
InP (mp-20351) <1 0 0> <1 0 0> 0.429 313.2
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.478 313.2
KCl (mp-23193) <1 1 0> <1 1 0> 0.490 177.2
C (mp-48) <1 1 0> <1 1 0> 0.506 265.8
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.551 187.9
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.572 250.6
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.577 62.6
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.598 313.2
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.637 62.6
TbScO3 (mp-31119) <0 1 0> <1 1 0> 0.641 88.6
InAs (mp-20305) <1 0 0> <1 0 0> 0.654 313.2
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.677 62.6
WS2 (mp-224) <1 1 1> <1 0 0> 0.690 313.2
Si (mp-149) <1 1 1> <1 0 0> 0.708 313.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
366 158 158 0 0 0
158 366 158 0 0 0
158 158 366 0 0 0
0 0 0 119 0 0
0 0 0 0 119 0
0 0 0 0 0 119
Compliance Tensor Sij (10-12Pa-1)
3.7 -1.1 -1.1 0 0 0
-1.1 3.7 -1.1 0 0 0
-1.1 -1.1 3.7 0 0 0
0 0 0 8.4 0 0
0 0 0 0 8.4 0
0 0 0 0 0 8.4
Shear Modulus GV
113 GPa
Bulk Modulus KV
228 GPa
Shear Modulus GR
112 GPa
Bulk Modulus KR
228 GPa
Shear Modulus GVRH
113 GPa
Bulk Modulus KVRH
228 GPa
Elastic Anisotropy
0.02
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Mg2H6Os (mp-643002) 0.0997 0.000 3
Zr2BIr6 (mp-1078623) 0.0027 0.000 3
Ir(Br3O)2 (mp-1079118) 0.1022 1.061 3
Se(Br3O)2 (mp-1079970) 0.0307 1.230 3
Pb(NCl3)2 (mp-1079281) 0.1081 1.198 3
LiMgH6Ir (mp-866640) 0.2394 0.000 4
Rb19O3 (mp-779582) 0.6631 0.043 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv B Rh_pv
Final Energy/Atom
-8.0804 eV
Corrected Energy
-72.7236 eV
-72.7236 eV = -72.7236 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 415337
Submitted by
User remarks:
  • Dititanium hexarhodium boride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)