material

MnSbRh2

ID:

mp-571163

DOI:

10.17188/1276114


Tags: Manganese rhodium antimonide (1/2/1)

Material Details

Final Magnetic Moment
4.184 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.291 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.046 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.07 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
MnRh + SbRh
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/mmm [123]
Hall
-P 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 76202 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TePb (mp-19717) <1 0 0> <0 0 1> 0.000 86.3
PbSe (mp-2201) <1 0 0> <0 0 1> 0.001 155.3
Ag (mp-124) <1 0 0> <0 0 1> 0.008 17.3
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.009 86.3
GaSb (mp-1156) <1 0 0> <0 0 1> 0.012 155.3
GaTe (mp-542812) <0 0 1> <1 0 0> 0.012 75.9
NdGaO3 (mp-3196) <1 1 0> <1 0 1> 0.013 183.9
GaTe (mp-542812) <1 0 1> <1 0 0> 0.013 197.4
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.017 138.0
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.025 224.3
CdSe (mp-2691) <1 0 0> <0 0 1> 0.028 155.3
GaTe (mp-542812) <1 0 -1> <1 0 0> 0.028 75.9
SrTiO3 (mp-4651) <1 0 1> <1 0 1> 0.040 160.9
SiO2 (mp-6930) <1 0 0> <1 0 1> 0.044 137.9
CaF2 (mp-2741) <1 0 0> <1 0 1> 0.045 91.9
CsI (mp-614603) <1 0 0> <1 0 1> 0.056 183.9
Au (mp-81) <1 0 0> <0 0 1> 0.057 17.3
SiO2 (mp-6930) <1 1 0> <1 1 1> 0.066 192.8
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.067 197.4
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.070 138.0
LaF3 (mp-905) <1 1 1> <1 0 1> 0.074 206.8
SiC (mp-11714) <1 0 1> <0 0 1> 0.078 258.8
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.082 120.8
LaF3 (mp-905) <1 0 1> <1 0 0> 0.085 212.5
GaP (mp-2490) <1 0 0> <1 0 1> 0.100 91.9
Bi2Se3 (mp-541837) <1 0 1> <1 0 1> 0.102 252.8
Mg (mp-153) <1 1 0> <1 0 1> 0.108 114.9
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.113 303.0
TiO2 (mp-390) <1 0 0> <0 0 1> 0.114 258.8
SiC (mp-8062) <1 0 0> <0 0 1> 0.117 155.3
SrTiO3 (mp-4651) <0 0 1> <1 0 1> 0.122 91.9
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.133 155.3
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.135 86.3
C (mp-48) <1 0 0> <1 1 0> 0.147 171.8
Ge3(BiO3)4 (mp-23560) <1 0 0> <0 0 1> 0.155 224.3
Mg (mp-153) <1 1 1> <1 0 1> 0.158 91.9
Te2W (mp-22693) <0 0 1> <1 0 0> 0.161 242.9
CdS (mp-672) <1 1 0> <1 1 0> 0.165 150.3
GaSe (mp-1943) <0 0 1> <1 0 1> 0.166 137.9
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.178 155.3
TiO2 (mp-2657) <1 1 1> <1 0 1> 0.178 206.8
Ag (mp-124) <1 1 0> <0 0 1> 0.180 120.8
Ni (mp-23) <1 1 0> <1 1 1> 0.180 192.8
CdS (mp-672) <1 0 0> <0 0 1> 0.181 86.3
Mg (mp-153) <0 0 1> <1 0 0> 0.187 60.7
InP (mp-20351) <1 1 0> <1 1 0> 0.188 150.3
InP (mp-20351) <1 1 1> <1 0 0> 0.190 60.7
NdGaO3 (mp-3196) <0 0 1> <1 0 1> 0.194 91.9
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.196 64.4
Al2O3 (mp-1143) <0 0 1> <1 0 0> 0.202 60.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
246 140 140 0 0 0
140 229 105 0 0 0
140 105 229 0 0 0
0 0 0 86 0 0
0 0 0 0 72 0
0 0 0 0 0 72
Compliance Tensor Sij (10-12Pa-1)
7.8 -3.3 -3.3 0 0 0
-3.3 6.9 -1.2 0 0 0
-3.3 -1.2 6.9 0 0 0
0 0 0 11.6 0 0
0 0 0 0 13.8 0
0 0 0 0 0 13.8
Shear Modulus GV
67 GPa
Bulk Modulus KV
164 GPa
Shear Modulus GR
64 GPa
Bulk Modulus KR
161 GPa
Shear Modulus GVRH
65 GPa
Bulk Modulus KVRH
163 GPa
Elastic Anisotropy
0.30
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
GaCuPt2 (mp-644280) 0.0961 0.000 3
VSnRh2 (mp-669918) 0.2198 0.011 3
CoSnRh2 (mp-1018085) 0.0269 0.060 3
CrSnRh2 (mp-1018066) 0.0994 0.000 3
AlCuPt2 (mp-12550) 0.0233 0.000 3
CrFeCoNi (mp-1012640) 0.7388 0.065 4
Yb3Tc (mp-979938) 0.0388 0.411 2
PmF3 (mp-862901) 0.0269 0.000 2
HgPd (mp-2685) 0.0169 0.000 2
Hf2Ag (mp-13155) 0.0301 0.000 2
Ge3Rh (mp-973883) 0.0100 0.365 2
Hg (mp-975272) 0.6213 0.001 1
K (mp-972981) 0.6052 0.008 1
Hg (mp-569360) 0.5552 0.001 1
W (mp-1065340) 0.6447 0.491 1
Eu (mp-1057315) 0.6139 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mn_pv Sb Rh_pv
Final Energy/Atom
-7.2962 eV
Corrected Energy
-29.1847 eV
-29.1847 eV = -29.1847 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 76202
Submitted by
User remarks:
  • Manganese rhodium antimonide (1/2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)