Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.764 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.76 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21/c [14]
Hall
-P 2ybc
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 58406 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
AlN (mp-661) <0 0 1> <0 0 1> 0.002 126.9
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.003 65.9
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.005 317.3
GaAs (mp-2534) <1 0 0> <1 0 0> 0.009 65.9
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.012 253.9
KCl (mp-23193) <1 0 0> <1 0 0> 0.016 329.3
GaP (mp-2490) <1 1 1> <0 0 1> 0.019 317.3
Cu (mp-30) <1 0 0> <1 0 0> 0.019 65.9
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.020 329.3
AlN (mp-661) <1 0 1> <1 0 0> 0.026 197.6
C (mp-48) <0 0 1> <0 1 0> 0.026 179.0
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.026 263.4
Ge (mp-32) <1 0 0> <1 0 0> 0.031 65.9
Al (mp-134) <1 0 0> <1 0 0> 0.032 65.9
Si (mp-149) <1 1 0> <0 0 1> 0.034 126.9
MgO (mp-1265) <1 0 0> <1 0 0> 0.035 329.3
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.035 126.9
NdGaO3 (mp-3196) <0 1 0> <0 0 1> 0.035 126.9
GaN (mp-804) <1 0 0> <0 0 1> 0.037 253.9
TiO2 (mp-390) <0 0 1> <1 0 0> 0.039 131.7
SiC (mp-7631) <0 0 1> <0 1 0> 0.039 298.4
SiC (mp-8062) <1 1 1> <1 0 -1> 0.040 299.6
NaCl (mp-22862) <1 1 1> <1 0 -1> 0.040 224.7
MgF2 (mp-1249) <1 0 1> <1 1 0> 0.044 266.6
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.044 317.3
BN (mp-984) <1 0 1> <1 0 0> 0.048 263.4
AlN (mp-661) <1 1 1> <0 0 1> 0.052 253.9
TiO2 (mp-2657) <1 0 0> <0 1 0> 0.053 179.0
CdS (mp-672) <1 0 0> <0 0 1> 0.053 317.3
Fe2O3 (mp-24972) <0 0 1> <1 0 -1> 0.055 299.6
C (mp-48) <1 0 0> <0 0 1> 0.056 190.4
Ni (mp-23) <1 1 0> <0 1 0> 0.057 298.4
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.065 65.9
LiF (mp-1138) <1 0 0> <1 0 0> 0.066 65.9
ZnO (mp-2133) <0 0 1> <0 1 1> 0.067 261.4
MgAl2O4 (mp-3536) <1 1 0> <0 0 1> 0.067 190.4
BN (mp-984) <1 1 0> <0 1 0> 0.070 298.4
LiF (mp-1138) <1 1 0> <0 0 1> 0.074 190.4
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.076 329.3
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.076 65.9
LiAlO2 (mp-3427) <1 0 1> <0 0 1> 0.081 126.9
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.083 253.9
C (mp-48) <1 1 1> <1 1 0> 0.084 266.6
PbS (mp-21276) <1 0 0> <1 0 0> 0.084 329.3
TiO2 (mp-390) <1 1 0> <0 0 1> 0.086 317.3
SiO2 (mp-6930) <1 0 0> <1 1 -1> 0.089 191.5
ZrO2 (mp-2858) <1 1 -1> <1 0 -1> 0.091 224.7
C (mp-48) <1 0 1> <1 0 0> 0.091 263.4
GaP (mp-2490) <1 1 0> <0 0 1> 0.092 126.9
NaCl (mp-22862) <1 0 0> <1 0 0> 0.098 65.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
58 35 29 0 -1 0
35 65 35 0 -3 0
29 35 60 0 -7 0
0 0 0 19 0 -0
-1 -3 -7 0 14 0
0 0 0 -0 0 19
Compliance Tensor Sij (10-12Pa-1)
27.3 -10.6 -7.6 0 -4 0
-10.6 26.5 -10.2 0 0.1 0
-7.6 -10.2 27.5 0 10.8 0
0 0 0 52.8 0 1.1
-4 0.1 10.8 0 78.8 0
0 0 0 1.1 0 52.3
Shear Modulus GV
16 GPa
Bulk Modulus KV
42 GPa
Shear Modulus GR
15 GPa
Bulk Modulus KR
41 GPa
Shear Modulus GVRH
16 GPa
Bulk Modulus KVRH
42 GPa
Elastic Anisotropy
0.30
Poisson's Ratio
0.33

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Y2Si4Mo3 (mp-2932) 0.2509 0.000 3
Tb2Ti3Si4 (mp-510083) 0.2367 0.000 3
Ho2Ti3Si4 (mp-510084) 0.2349 0.000 3
Er2Ti3Si4 (mp-510085) 0.2386 0.000 3
Dy2Ti3Si4 (mp-19950) 0.2487 0.000 3
La5Sn4 (mp-30757) 0.3127 0.000 2
Y5Pb4 (mp-672188) 0.2848 0.368 2
Tb5Ge4 (mp-1673) 0.3051 0.000 2
Y5Ge4 (mp-13360) 0.3133 0.000 2
Hf5Si4 (mp-17216) 0.2974 0.004 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Au
Final Energy/Atom
-3.3333 eV
Corrected Energy
-59.9988 eV
Uncorrected energy = -59.9988 eV Corrected energy = -59.9988 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 58406
Submitted by
User remarks:
  • Gold calcium (4/5)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)