Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.187 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.133 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNb3Ge |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 254.0 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 167.7 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 215.6 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 119.8 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 215.6 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 191.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 152.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 263.5 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 205.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 33.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 47.9 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 169.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 152.4 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 215.6 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 205.3 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 117.3 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 263.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 203.2 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 271.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 88.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 304.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 287.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 287.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 215.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 84.7 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 205.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 95.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 135.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 215.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 47.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 191.6 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 47.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 16.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 24.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 29.3 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 118.5 |
CdS (mp-672) | <1 1 0> | <1 1 1> | 352.0 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 271.0 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 24.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 167.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 152.4 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 215.6 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 205.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 33.9 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 169.4 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 215.6 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 287.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 84.7 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 167.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 16.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
74 | 129 | 129 | 0 | 0 | 0 |
129 | 74 | 129 | 0 | 0 | 0 |
129 | 129 | 74 | 0 | 0 | 0 |
0 | 0 | 0 | 77 | 0 | 0 |
0 | 0 | 0 | 0 | 77 | 0 |
0 | 0 | 0 | 0 | 0 | 77 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-11.1 | 7.1 | 7.1 | 0 | 0 | 0 |
7.1 | -11.1 | 7.1 | 0 | 0 | 0 |
7.1 | 7.1 | -11.1 | 0 | 0 | 0 |
0 | 0 | 0 | 13 | 0 | 0 |
0 | 0 | 0 | 0 | 13 | 0 |
0 | 0 | 0 | 0 | 0 | 13 |
Shear Modulus GV35 GPa |
Bulk Modulus KV111 GPa |
Shear Modulus GR-148 GPa |
Bulk Modulus KR111 GPa |
Shear Modulus GVRH-56 GPa |
Bulk Modulus KVRH111 GPa |
Elastic Anisotropy-6.19 |
Poisson's Ratio0.81 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.000 | 3 |
LiCa6Ge (mp-12609) | 0.0000 | 0.180 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.066 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
Hg3F (mp-973777) | 0.0000 | 0.170 | 2 |
NdPt3 (mp-569120) | 0.0000 | 0.017 | 2 |
HfPd3 (mp-1007656) | 0.0000 | 0.014 | 2 |
Pd3Au (mp-999298) | 0.0000 | 0.000 | 2 |
HfRh3 (mp-1027) | 0.0000 | 0.000 | 2 |
Sr (mp-76) | 0.0000 | 0.006 | 1 |
N2 (mp-1056857) | 0.0000 | 0.000 | 1 |
Ni (mp-1056486) | 0.0000 | 0.000 | 1 |
Cd (mp-1096861) | 0.0000 | 0.001 | 1 |
Pd (mp-1056438) | 0.0000 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv Ge_d |
Final Energy/Atom-8.9172 eV |
Corrected Energy-35.6687 eV
-35.6687 eV = -35.6687 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)