Final Magnetic Moment0.025 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.438 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/amd [141] |
HallI 4bw 2bw 1bw |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 77.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 356.1 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 136.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 31.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 154.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 77.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 170.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 170.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 340.7 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 136.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 216.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 309.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 232.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 61.9 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 294.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 77.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 139.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 15.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 136.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 139.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 247.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 371.6 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 201.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 139.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 263.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 232.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 77.4 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 216.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 77.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 325.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 201.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 216.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 139.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 356.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 247.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 247.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 77.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 325.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 278.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 340.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 278.7 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 232.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 201.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 278.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 278.7 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 278.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 139.4 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 263.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 123.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 77.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
196 | 71 | 59 | 0 | 0 | 0 |
71 | 196 | 59 | 0 | 0 | 0 |
59 | 59 | 189 | 0 | 0 | 0 |
0 | 0 | 0 | 68 | 0 | 0 |
0 | 0 | 0 | 0 | 68 | 0 |
0 | 0 | 0 | 0 | 0 | 79 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
6.2 | -1.8 | -1.4 | 0 | 0 | 0 |
-1.8 | 6.2 | -1.4 | 0 | 0 | 0 |
-1.4 | -1.4 | 6.1 | 0 | 0 | 0 |
0 | 0 | 0 | 14.8 | 0 | 0 |
0 | 0 | 0 | 0 | 14.8 | 0 |
0 | 0 | 0 | 0 | 0 | 12.7 |
Shear Modulus GV69 GPa |
Bulk Modulus KV107 GPa |
Shear Modulus GR69 GPa |
Bulk Modulus KR107 GPa |
Shear Modulus GVRH69 GPa |
Bulk Modulus KVRH107 GPa |
Elastic Anisotropy0.03 |
Poisson's Ratio0.23 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaMg6Mo (mp-1098241) | 0.2954 | 0.235 | 3 |
NaHfMg6 (mp-1098253) | 0.2951 | 0.153 | 3 |
CrFeCoNi (mp-1096923) | 0.7084 | 0.193 | 4 |
ZrGa2 (mp-30683) | 0.2648 | 0.000 | 2 |
ZrIn2 (mp-20800) | 0.1688 | 0.000 | 2 |
HfGa2 (mp-11440) | 0.1193 | 0.000 | 2 |
LaSn2 (mp-1077735) | 0.2806 | 0.014 | 2 |
ScGa2 (mp-11413) | 0.1021 | 0.023 | 2 |
Hg (mp-975272) | 0.6539 | 0.001 | 1 |
Tl (mp-972351) | 0.6723 | 0.000 | 1 |
Hg (mp-569360) | 0.6187 | 0.001 | 1 |
W (mp-1065340) | 0.5549 | 0.491 | 1 |
Cs (mp-1012110) | 0.5818 | 0.046 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv Ga_d |
Final Energy/Atom-5.0882 eV |
Corrected Energy-61.0588 eV
-61.0588 eV = -61.0588 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)