Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.384 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.13 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P6422 [181]
Hall
P 64 2c (0 0 1)
Point Group
622
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaSb (mp-1156) <1 1 1> <0 0 1> 0.000 268.1
PbSe (mp-2201) <1 1 1> <0 0 1> 0.003 268.1
WS2 (mp-224) <0 0 1> <0 0 1> 0.005 61.9
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.005 61.9
CdSe (mp-2691) <1 1 1> <0 0 1> 0.005 268.1
C (mp-66) <1 1 1> <1 1 0> 0.010 221.8
CaCO3 (mp-3953) <0 0 1> <1 1 0> 0.014 221.8
Ag (mp-124) <1 1 1> <0 0 1> 0.029 268.1
InP (mp-20351) <1 1 1> <0 0 1> 0.033 61.9
Mg (mp-153) <0 0 1> <0 0 1> 0.034 61.9
Te2W (mp-22693) <0 0 1> <1 1 0> 0.055 221.8
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.056 144.4
PbS (mp-21276) <1 1 1> <0 0 1> 0.056 61.9
CdS (mp-672) <0 0 1> <0 0 1> 0.063 61.9
CeO2 (mp-20194) <1 0 0> <1 0 1> 0.066 237.0
MgF2 (mp-1249) <1 1 1> <1 0 0> 0.069 298.8
Si (mp-149) <1 0 0> <1 0 1> 0.072 237.0
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.079 185.6
KCl (mp-23193) <1 1 0> <1 1 1> 0.079 230.3
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.084 330.0
Au (mp-81) <1 1 1> <0 0 1> 0.097 268.1
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.097 268.1
KP(HO2)2 (mp-23959) <0 0 1> <0 0 1> 0.103 226.9
C (mp-48) <1 1 1> <0 0 1> 0.108 268.1
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.112 144.4
InAs (mp-20305) <1 1 1> <0 0 1> 0.116 268.1
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.124 256.1
C (mp-48) <1 0 1> <1 0 1> 0.124 237.0
GaN (mp-804) <0 0 1> <0 0 1> 0.131 61.9
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.133 185.6
SiO2 (mp-6930) <1 1 1> <1 0 0> 0.134 213.4
ZrO2 (mp-2858) <0 1 1> <1 0 1> 0.142 237.0
MgO (mp-1265) <1 1 0> <0 0 1> 0.151 103.1
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.155 309.4
BaTiO3 (mp-5986) <1 1 1> <1 1 1> 0.165 230.3
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.166 309.4
KP(HO2)2 (mp-23959) <0 1 0> <0 0 1> 0.174 226.9
Te2W (mp-22693) <0 1 1> <1 1 0> 0.177 295.7
InAs (mp-20305) <1 1 0> <1 0 0> 0.180 213.4
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.196 61.9
ZnTe (mp-2176) <1 1 0> <1 0 0> 0.199 213.4
KTaO3 (mp-3614) <1 1 0> <1 0 0> 0.214 298.8
Al (mp-134) <1 1 0> <1 0 0> 0.217 298.8
C (mp-66) <1 0 0> <0 0 1> 0.238 226.9
C (mp-48) <1 1 0> <0 0 1> 0.240 268.1
Al2O3 (mp-1143) <1 0 0> <1 0 0> 0.241 128.1
Au (mp-81) <1 1 0> <0 0 1> 0.241 350.6
Al2O3 (mp-1143) <1 1 0> <1 1 0> 0.242 221.8
C (mp-66) <1 1 0> <1 0 0> 0.242 213.4
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.255 185.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
327 134 93 0 0 0
134 327 93 0 0 0
93 93 433 0 0 0
0 0 0 56 0 0
0 0 0 0 56 0
0 0 0 0 0 96
Compliance Tensor Sij (10-12Pa-1)
3.8 -1.4 -0.5 0 0 0
-1.4 3.8 -0.5 0 0 0
-0.5 -0.5 2.5 0 0 0
0 0 0 17.8 0 0
0 0 0 0 17.8 0
0 0 0 0 0 10.4
Shear Modulus GV
93 GPa
Bulk Modulus KV
192 GPa
Shear Modulus GR
80 GPa
Bulk Modulus KR
191 GPa
Shear Modulus GVRH
86 GPa
Bulk Modulus KVRH
192 GPa
Elastic Anisotropy
0.82
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
MgBIr (mp-569048) 0.3407 0.000 3
NaSi2Pd3 (mp-4276) 0.7127 0.000 3
MgZn2 (mp-567626) 0.7411 0.138 2
MgSi2 (mp-1073254) 0.7118 0.195 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Ni_pv B
Final Energy/Atom
-5.7661 eV
Corrected Energy
-103.7900 eV
Uncorrected energy = -103.7900 eV Corrected energy = -103.7900 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 156018
Submitted by
User remarks:
  • Magnesium nickel boride (1/3/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)