material

RbGeI3

ID:

mp-571458

DOI:

10.17188/1276270


Tags: High pressure experimental phase Rubidium triiodogermanate - HT

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.787 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.025 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.23 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
RbI + GeI2
Band Gap
0.554 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Mg (mp-153) <0 0 1> <1 1 1> 0.000 61.4
InP (mp-20351) <1 1 1> <1 1 1> 0.000 61.4
InP (mp-20351) <1 1 0> <1 1 0> 0.000 50.2
InP (mp-20351) <1 0 0> <1 0 0> 0.000 35.5
LiF (mp-1138) <1 0 0> <1 0 0> 0.000 283.8
Ni (mp-23) <1 0 0> <1 0 0> 0.001 319.3
CdS (mp-672) <0 0 1> <1 1 1> 0.002 61.4
Ge(Bi3O5)4 (mp-23352) <1 1 1> <1 1 1> 0.003 184.3
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 0.004 150.5
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.005 61.4
WS2 (mp-224) <0 0 1> <1 1 1> 0.005 61.4
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.010 319.3
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.011 248.3
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.012 319.3
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.012 177.4
InSb (mp-20012) <1 0 0> <1 0 0> 0.019 177.4
SiC (mp-8062) <1 1 0> <1 1 0> 0.022 301.0
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.025 61.4
C (mp-66) <1 1 0> <1 1 0> 0.026 200.7
CdTe (mp-406) <1 0 0> <1 0 0> 0.026 177.4
AlN (mp-661) <1 0 1> <1 1 0> 0.031 250.9
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.034 319.3
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.037 319.3
AlN (mp-661) <1 1 1> <1 1 0> 0.039 200.7
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.039 184.3
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.039 184.3
YVO4 (mp-19133) <1 0 0> <1 1 1> 0.041 184.3
LaF3 (mp-905) <0 0 1> <1 1 1> 0.048 184.3
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.049 212.9
AlN (mp-661) <1 1 0> <1 1 0> 0.052 301.0
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.058 177.4
BaTiO3 (mp-5986) <1 0 0> <1 1 1> 0.061 307.2
MgO (mp-1265) <1 1 1> <1 0 0> 0.061 248.3
GaN (mp-804) <1 0 1> <1 0 0> 0.067 212.9
PbS (mp-21276) <1 1 1> <1 1 1> 0.068 61.4
ZnO (mp-2133) <1 1 1> <1 0 0> 0.068 283.8
PbS (mp-21276) <1 1 0> <1 1 0> 0.070 50.2
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.073 283.8
Bi2Se3 (mp-541837) <1 0 0> <1 0 0> 0.074 248.3
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.077 141.9
PbS (mp-21276) <1 0 0> <1 0 0> 0.078 35.5
GaN (mp-804) <0 0 1> <1 1 0> 0.079 250.9
Cu (mp-30) <1 1 0> <1 1 0> 0.081 150.5
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.081 150.5
Ni (mp-23) <1 1 0> <1 1 0> 0.083 301.0
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.090 283.8
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.097 200.7
Au (mp-81) <1 1 0> <1 1 0> 0.103 50.2
Au (mp-81) <1 0 0> <1 0 0> 0.114 35.5
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.114 177.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
40 7 7 0 0 0
7 40 7 0 0 0
7 7 40 0 0 0
0 0 0 8 0 0
0 0 0 0 8 0
0 0 0 0 0 8
Compliance Tensor Sij (10-12Pa-1)
26.1 -3.8 -3.8 0 0 0
-3.8 26.1 -3.8 0 0 0
-3.8 -3.8 26.1 0 0 0
0 0 0 132 0 0
0 0 0 0 132 0
0 0 0 0 0 132
Shear Modulus GV
11 GPa
Bulk Modulus KV
18 GPa
Shear Modulus GR
10 GPa
Bulk Modulus KR
18 GPa
Shear Modulus GVRH
10 GPa
Bulk Modulus KVRH
18 GPa
Elastic Anisotropy
0.79
Poisson's Ratio
0.26

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ba2ScSbO6 (mp-20709) 0.0000 2.196 4
Sr2GaSbO6 (mp-6065) 0.0003 0.039 4
YbBa2SbO6 (mp-14223) 0.0000 1.748 4
Ba2YSbO6 (mp-14226) 0.0000 2.084 4
Cs2LiYCl6 (mp-567652) 0.0001 0.000 4
Mn4N (mp-505622) 0.0000 0.000 2
Sr3N2 (mp-1013529) 0.0000 0.557 2
Sr3As2 (mp-1013559) 0.0000 0.370 2
Ba3Sb2 (mp-1013582) 0.0000 0.415 2
Ba3P2 (mp-1013551) 0.0000 0.447 2
MnTlCl3 (mp-570290) 0.0000 0.029 3
AcCrO3 (mp-866647) 0.0000 0.000 3
HgIrO3 (mp-1016831) 0.0000 0.405 3
MgMnO3 (mp-976446) 0.0000 0.492 3
CaZrO3 (mp-542112) 0.0000 0.192 3
SrLaNbZnO6 (mp-41918) 0.0385 0.126 5
BaLaMgBiO6 (mp-41414) 0.0288 0.095 5
BaCaLaBiO6 (mp-39886) 0.0711 0.154 5
BaLaTaZnO6 (mp-42054) 0.0630 0.111 5
BaLaMgTaO6 (mp-40251) 0.0443 0.080 5
Ba3LaZnReWO12 (mp-705508) 0.6831 0.059 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Rb_sv Ge_d I
Final Energy/Atom
-2.8166 eV
Corrected Energy
-14.0832 eV
-14.0832 eV = -14.0832 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 40216
Submitted by
User remarks:
  • High pressure experimental phase
  • Rubidium triiodogermanate - HT

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)